CSN 423063

Quick Comparison

Wrought Copper Nickel Grade

EN 1652 Grade CuNi30Mn1Fe R350

Wrought Copper Nickel Grade

EN 1652 Grade CuNi30Mn1Fe R410

Wrought Copper Nickel Grade

EN 12163 Grade CuNi30Mn1Fe R420

Wrought Copper Nickel Grade

EN 1652 Grade CuNi30Mn1Fe H080

Wrought Copper Nickel Grade

EN 12163 Grade CuNi30Mn1Fe R340

Wrought Copper Nickel Grade

EN 1652 Grade CuNi30Mn1Fe H110

Wrought Copper Nickel Grade

EN 12163 Grade CuNi30Mn1Fe M