Wrought Copper Nickel Silver Grade
CEN/TS 13388 Grade CW408J R420Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn38Mn5Pb2 H150Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn38Mn5Pb2 H170Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn38Mn5Pb2 R600Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn38Mn5Pb2 R650Wrought Copper Nickel Grade
EN 1652 Grade CuNi25 R290Wrought Copper Nickel Grade
EN 1652 Grade CuNi25 H070Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn38Mn5Pb2 MWrought Copper Nickel Silver Grade
DIN 17663 Grade 2.0750Wrought Copper Nickel Grade
GB 5234 Grade B25Wrought Copper Nickel Grade
AS/NZS 2738 Grade 713Wrought Copper Nickel Grade
CEN/TS 13388 Grade C-7310Wrought Copper Nickel Grade
ISO 429 Grade CuNi25Wrought Copper Nickel Grade
BS 2870 Grade CW350HWrought Copper Nickel Grade
CEN/TS 13388 Grade CuNi25Wrought Copper Nickel Grade
MSZ 771-1 Grade CW350HWrought Copper Nickel Grade
NP 3641 Grade CW350HWrought Copper Nickel Grade
PN/H 87052 Grade CW350HWrought Copper Nickel Grade
CEN/TS 13388 Grade CW350HWrought Copper Nickel Grade
BS 2873 Grade NS 109