Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10028-7 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable ferrítico
EN 10028-7 Grade X2CrMoTi18-2 soft annealed (+A)Acero inoxidable austenítico
EN 10216-5 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10217-7 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10250-4 Grade X3CrNiMo17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10250-4 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10270-3 Grade X5CrNiMo17-12-2 cold drawnAcero inoxidable austenítico
EN 10222-5 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10269 Grade X5CrNiMo17-12-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10269 Grade X5CrNiMo17-12-2 strain-hardened (+C700)Acero inoxidable austenítico
DIN 5512-3 Grade X5CrNiMo17-12-2 strain-hardened (+C700)Acero inoxidable austenítico
EN 10088-1 Grade X5CrNiMo17-12-2 strain-hardened (+C700)Acero inoxidable ferrítico
EN 10028-7 Grade X2CrMoTi18-2 solution annealed (+AT)