ISO CuAl10Fe3

Quick Comparison

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Wrought Copper Bronze Aluminium Bronze

EN 12165 Grade CuAl10Fe3Mn2 H120

Wrought Copper Bronze Aluminium Bronze

EN 12163 Grade CuAl10Fe3Mn2 R590

Wrought Copper Bronze Aluminium Bronze

EN 12163 Grade CuAl10Fe3Mn2 R690

Wrought Copper Bronze Aluminium Bronze

EN 12163 Grade CuAl10Fe3Mn2 H140

Wrought Copper Bronze Aluminium Bronze

EN 12163 Grade CuAl10Fe3Mn2 H170

Wrought Copper Bronze Aluminium Bronze

EN 12167 Grade CuAl10Fe3Mn2 H130

Wrought Copper Bronze Aluminium Bronze

EN 12167 Grade CuAl10Fe3Mn2 H160

Wrought Copper Bronze Aluminium Bronze

EN 12167 Grade CuAl10Fe3Mn2 R550

Wrought Copper Bronze Aluminium Bronze

EN 12167 Grade CuAl10Fe3Mn2 R650

Wrought Copper Bronze Aluminium Bronze

EN 12165 Grade CuAl10Fe3Mn2 M

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C62300 HR50

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C62300 M20

Wrought Copper Bronze Aluminium Bronze

ASTM B150 Grade C62300 M20

Wrought Copper Bronze Aluminium Bronze

BS CA103 Bronze

Cast Copper Bronze Aluminium Bronze

ASTM B148 Grade C95200 As-Cast

Cast Copper Bronze Aluminium Bronze

ASTM B271 Grade C95200 As-Cast

Cast Copper Bronze Aluminium Bronze

ASTM B763 Grade C95200 Separately Cast Test Bars

Wrought Copper Bronze Aluminium Bronze

JIS H3100 Grade C6161 H02

Wrought Copper Bronze Aluminium Bronze

JIS H3100 Grade C6161 O
Página 1 de 2