General
Property | Value | Comment |
---|---|---|
Density | 7.677 g/cm³ Show Material materials with Density of 7.677 g/cm³ | Predicted Value |
Grain size | 0.0293 μm Show Material materials with Grain size of 0.0293 μm | Predicted Value |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Compressive strength | 1201 MPa Show Material materials with Compressive strength of 1201 MPa | Predicted Value | ||
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Fatigue strength | 404 MPa Show Material materials with Fatigue strength of 404 MPa | Predicted Value | ||
Hardness, Brinell | 141 [-] Show Material materials with Hardness, Brinell of 141 [-] | Predicted Value | ||
Hardness, HBW | 259.7 [-] Show Material materials with Hardness, HBW of 259.7 [-] | Predicted Value | ||
Hardness, Rockwell F | 75 [-] Show Material materials with Hardness, Rockwell F of 75 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 70 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 70 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | Predicted Value | ||
Hardness, Vickers | 143 [-] Show Material materials with Hardness, Vickers of 143 [-] | Predicted Value | ||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze | ||
Reduction of area | 47.0 % Show Material materials with Reduction of area of 47.0 % | Predicted Value | ||
Shear modulus | 43.5 GPa Show Material materials with Shear modulus of 43.5 GPa | Predicted Value | ||
Shear strength | 317.8 MPa Show Material materials with Shear strength of 317.8 MPa | Predicted Value | ||
Tensile strength | 469 MPa Show Material materials with Tensile strength of 469 MPa | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Electrical
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 8.5 - 9.5 % Show Material materials with Aluminium of 8.5 - 9.5 % | ASTM B505 | Casting |
Copper | 86 % Show Material materials with Copper of 86 % | ASTM B505 | Casting |
Iron | 2.5 - 4 % Show Material materials with Iron of 2.5 - 4 % | ASTM B505 | Casting |