Acero inoxidable austenítico
Sandvik 5R10Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10028-7 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNi18-11 solution annealed (+AT)Acero inoxidable austenítico
EN 10216-5 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10222-5 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
DIN 17460 Grade X6CrNi18-11 solution annealed (+AT)Acero inoxidable austenítico
EN 10269 Grade X6CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
ASTM A213 Grade TP304H Heat-TreatedAcero inoxidable austenítico
ASTM A249 Grade TP304H Heat-TreatedAcero inoxidable austenítico
ASTM A240 Grade 304H Heat-TreatedAcero inoxidable austenítico
ASTM A182 Grade F304H Solution-AnnealedAcero inoxidable austenítico
ASTM A479 Grade 304H AnnealedAcero inoxidable austenítico
ASTM A965 Grade F304H Solution-TreatedAcero inoxidable austenítico
JIS G3459 Grade SUS304HTPAcero inoxidable austenítico
JIS G3463 Grade SUS304HTBAcero inoxidable austenítico
JIS G3467 Grade SUS304HTFAcero inoxidable austenítico
ASTM A312 Grade TP304HAcero inoxidable austenítico
ASTM A403 Grade S30409 Heat-TreatedAcero inoxidable austenítico
ASTM A376 Grade TP304H Heat-TreatedAcero inoxidable austenítico
ASTM A813 Grade TP304H Solution-Treated