Density ρ
7.9 - 8.2 g/cm³ at 20 °C
Typical for Austenitic Stainless Steel
Poisson's ratio ν
0.3 [-] at 20 °C
Typical for Austenitic Stainless Steel
Tensile strength Rm
0 - 515 MPa at 20 °C
Yield strength YS
0 - 205 MPa at 20 °C
Coefficient of thermal expansion α
1.7E-5 - 1.9E-5 1/K at 20 °C
Typical for Austenitic Stainless Steel
Melting point Tm
1375 - 1450 °C
Typical for Austenitic Stainless Steel
Thermal conductivity λ
11 - 21 W/(m·K) at 20 °C
Typical for Austenitic Stainless Steel
Element
Weight %
Comment
18 - 20 %
8 - 11 %
0.04 - 0.1 %
0 - 2 %
0 - 0.05 %
This material data has been provided by ASTM.