ASTM A668

Quick Comparison

Medium Carbon Steel

ASTM A668 Class A Untreated

Nickel Chromium Molybdenum Steel

ASTM A668 Class H Normalized and tempered

Unclassified Low Alloy Steel

ASTM A668 Class HH Normalized and tempered
Página 1 de 2