General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 19 - 20 % Show Material materials with Elongation A50 of 19 - 20 % | |
Hardness, Brinell | 23.0 °C | 174 - 235 [-] Show Material materials with Hardness, Brinell of 174 - 235 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 36 - 39 % Show Material materials with Reduction of area of 36 - 39 % | |
Tensile strength | 23.0 °C | 565 - 620 MPa Show Material materials with Tensile strength of 565 - 620 MPa | |
Yield strength | 23.0 °C | 330 - 380 MPa Show Material materials with Yield strength of 330 - 380 MPa |