General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Elongation A50 | 20.0 °C | 18 - 20 % Show Material materials with Elongation A50 of 18 - 20 % | |
Hardness, Brinell | 20.0 °C | 207 - 269 [-] Show Material materials with Hardness, Brinell of 207 - 269 [-] | |
Poisson's ratio | 20.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Reduction of area | 20.0 °C | 48 - 50 % Show Material materials with Reduction of area of 48 - 50 % | |
Tensile strength | 20.0 °C | 690 - 725 MPa Show Material materials with Tensile strength of 690 - 725 MPa | |
Yield strength | 20.0 °C | 515 - 550 MPa Show Material materials with Yield strength of 515 - 550 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Thermal conductivity | 20.0 °C | 34 - 54 W/(m·K) Show Material materials with Thermal conductivity of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |