LDPE vs HDPE: Properties, Production and Applications

LDPE and HDPE are thermoplastic materials under the family of polyolefins, which are petrochemical-based plastics that include polypropylene (PP) and polyethylene (PE). Polyethylene is the most common plastic material in the world and is known for its simple structure, the simplest of all polymers commercially available.

Collectively under the polyethylene class of materials, LDPE (low-density polyethylene) and HDPE (high-density polyethylene) have shaped the landscape of the packaging and manufacturing industry. LDPE is well known for being widely used in plastic bags as its low density makes it light and flexible, rendering it perfect for this kind of application. HDPE, on the other hand, is harder and offers higher strength and better resistance to heat. Recently, it has become very popular as a source material for 3D printing filaments, used instead of ABS material. It is also used to produce durable plastic parts such as HDPE pipes, toys and plastic chairs.

Although LDPE and HDPE are both thermoplastic ethylene polymers, they differ in several properties and uses. One stark contrast is that LDPE has more branching than HDPE. Branching takes place during polymerisation, where polymer chains have secondary polymer chains attached to them by replacing an atom in the primary chain with a monomer group. This weakens the intermolecular forces in the polymer. That is why HDPE have a higher strength-to-density ratio than LDPE with increased tensile strength.

The varying uses of LDPE and HDPE are based on this fundamental structural difference, among many other properties.

Here, you will learn about:

  • The divergence in properties between LDPE and HDPE

  • The advantages and disadvantages of using each polyethylene material

  • How each of them is produced and processed

  • The different applications of LDPE and HDPE

LDPE plastic bags tied next to each other

LDPE plastic bags

Properties of LDPE and HDPE

Although both materials come from the same ethylene monomer, the difference in chemical structure yields a wide variety of unique properties.

As its name suggests, low-density polyethylene (LDPE) has a lower density, strength, and temperature resistance. Meanwhile, high-density polyethylene (HDPE) is characterized by higher specific strength and heat resistance.

Table 1. Comparison of the material properties of LDPE and HDPE

Property

LDPE

HDPE

Chemical structure

More branching

Less branching, more linear

Density

Low density

0.91-0.94 g/cm3

High density

0.95-0.97 g/cm3

Flexibility

Low crystallinity (50-60%), and therefore more flexible

High crystallinity (>90%), which makes it tougher and more rigid

Heat resistance

Drastic decrease in density when subjected to temperatures beyond 20°C

Able to withstand heat with temperatures more than 100°C

Melting point

~115°C

~135°C

Chemical resistance

Resistant to most alcohols, acids, and alkalis; low resistance to oxidising agents and selected hydrocarbons

Superior resistance to solvents, alcohols, acids, and alkalis; low resistance to most hydrocarbons

Strength

Relatively increased impact strength in cold conditions

High tensile and specific strength

Transparency

High, due to amorphous condition

Low, due to increased level of crystallinity

Maximum allowable stress at 20°C

6–17 MPa

14–32 MPa

Pros and cons of using LDPE and HDPE

While both materials have their respective benefits, they also carry with them a number of disadvantages. Here's a list of the pros and cons of each of LDPE and HDPE.

Table 2. Advantages and disadvantages of using LDPE vs HDPE

 

LDPE

HDPE

Advantages

Wide variety of uses

Low cost

Resistant to acids and bases

Easy to process and mould

Good electrical insulation

Waterproof property

May be processed as transparent

Wide variety of uses

Low cost

High tensile strength

Able to resist low temperature

Relatively strong and stiff

Waterproof property

Good electrical insulation

Disadvantages

More prone to crack stress

Not useful in extremely high or low temperatures

High permeability to carbon dioxide and other gases

Little to no UV resistance

May crack under stress

Higher risk of mould shrinking

Little to no UV resistance

 

 

 

Discover different LDPE and HDPE materials on Matmatch

Production and processing of LDPE and HDPE

How is LDPE produced?

LDPE is made through either a stirred autoclave or tubular reactor. Its general manufacture involves the compression of ethylene gas, polymerisation using an initiator, and gas separation.

How is HDPE produced?

Most HDPE materials are produced by either slurry polymerisation or gas phase polymerisation. The process starts with polymerisation from a solution of ethylene monomers, followed by separation and drying.

How are those two polyethylene materials processed?

Once produced, the thermoplastic material may be processed for consumer or industrial use by the following methods:

Injection moulding

This rapid process converts LDPE and HDPE pellets or granules into custom shapes and sizes defined by the mould. The thermoplastic pellets are sent to a hot barrel, from which the materials are melted through a screw barrel and heater bands. The molten plastic is then injected to a pre-configured mould cavity, which also cools down the material. After solidifying, the plastic material is ejected out of the moulding machine.

 

Extrusion

Similar to injection moulding, this also makes use of heat to melt the plastic granules. The difference comes at the final section of the machine – in this case, the melted plastic goes through a pre-designed opening and is then cooled down to solidify.

 

Blow moulding

This type of processing is usually carried out to manufacture hollow-shaped plastic goods. Instead of injecting the molten plastic, the process uses compressed air to blow the material into the mould.

Black HDPE pipes

HDPE pipes

Applications of LDPE and HDPE

LDPE applications include:

  • LDPE plastic bags
  • Light packaging materials: Six-pack rings, waterproof carton lining, plastic wraps, snap-on lids
  • Wash bottles
  • Corrosion protection layer for work surfaces
  • Computer hardware covers and packaging

HDPE applications include:

  • HDPE filament for 3D printers
  • Strong packaging materials: bottle caps, plastic milk bottles, drums, bulk containers for industrial use
  • Fibres for ropes, nets, and industrial fabrics
  • Vehicle fuel tanks
  • Boat parts
  • HDPE pipes and tubing
  • HDPE plastic chairs and tables
  • Playground structures: slides, swing seats
  • Consumer products: trash and recycling bins, ice cube containers, toys, ice chests

Discover different LDPE and HDPE materials on Matmatch

 

If you've enjoyed reading this article, you can also read more related content here:

Fuentes

[1] S.T. Sam, M.A. Nuradibah, H. Ismail, N.Z. Noriman, S. Ragunathan, "Recent Advances in Polyolefins/Natural Polymer Blends Used for Packaging Application", Polymer-Plastics Technology and Engineering, 53:6, pp. 631-44, 2014.

[2] A. Peacock, Handbook of Polyethylene: Structures, Properties, and Applications, NY: Marcel Dekker, Inc., 2000.

[3] NIIR Board of Consultants and Engineers, The Complete Technology Book on Plastic Films, HDPE and Thermoset Plastics, India: Asia Pacific Business Press, Inc., 2006.

[4] "Highlights of Low-Density Polyethylene", [Online] Available from: https://www.plasticsmakeitpossible.com/about-plastics/faqs/professor-plastics/professor-plastics-highlights-of-low-density-polyethylene/

[5] Yashoda, "Difference Between HDPE and LDPE", [Online] Available from: http://pediaa.com/difference-between-hdpe-and-ldpe/, 2016.

[6] J.P. Plog, "Processing Polyethylene", [Online] Available from: https://www.thermofisher.com/blog/materials/processing-polyethylene/, 2015.