The Radel® R-5100 is a registered trademark of the Solvay specialty polymers division. This engineering resin is a general purpose injection moulding grade belonging to the polyphenylsulfone (PPSU) series of the sulfone polymer family. This series stands out as the highest performance of other sulfone polymers, offering good resistance to hydrolysis, high heat deflection temperature, and enhanced impact resistance and outstanding chemical resistance. These thermoplastics are inherently flame retardant.

Here, you will learn about:

  • What sulfone polymers are
  • Key features and properties of Radel® R-5100
  • How Radel® R-5100 is processed
  • Applications of Radel® R-5100

The chemistry and properties of Radel® R-5100

Fig 1. Monomeric unit of Radel® PPSU

The Radel® R-5100 is an amorphous thermoplastic with no distinct melting point and lacks crystallinity. Polysulfone polymers contain linked phenyl groups joined by sulfone (-SO2-) groups. The sulfone functional group provides inherent hydrolytic stability, as the hexavalent sulfur atom is in its highest oxidation state. Additionally, the sulfone functional group is surrounded on each side by a phenyl substituent, and the resulting diaryl sulfone further increases the inherent hydrolytic stability of the sulfone group. 

In Radel® PPSU, the biphenyl moiety confers additional stability and extends the aromaticity throughout. This directly translates into a significantly increased impact strength value (notched Izod greater than 690 J/m) that is significantly higher than other sulfone polymers. On each side of the biphenyl is an oxygen atom that results in a phenolic ether moiety, adding flexibility to the polymer chain with the resulting properties of higher toughness, elongation, and ductility.

 

Key features and properties of Radel® R-5100

Exceptional hydrolytic stability

Superior toughness

High deflection temperature

Resistance to environmental stress cracking

Flame retardant

Excellent thermal stability

Good electrical properties

 

Similar grades to Radel® R-5100 and colourability

Naturally opaque, the R-5100 may be easily coloured and is available in a variety of hues including:

Colour

 

Designation

Black 

image.png Radel® R-5100 BK937
Bone  

image.png

Radel® R-5100 NT15

Grey 

image.png

Radel® R-5100 GY1137

Grey 

image.png

Radel® R-5100 GY1037

Grey 

image.png

Radel® R-5100 GY874

Red 

image.png

Radel® R-5100 RD1018

Orange 

image.png

Radel® R-5100 OR1145

Yellow 

image.png

Radel® R-5100 YL1337

Green 

image.png

Radel® R-5100 GN1007

Blue 

image.png

Radel® R-5100 BU1027

Violet 

image.png

Radel® R-5100 VT2582

Brown 

image.png

Radel® R-5100 RD1018

 

The similar general purpose grade for injection moulding R-5000 is transparent. Additional grades in the series include a transparent grade R-5500 for extrusion, higher flow transparent grades R-5800 and R-5900 for injection moulding, and a 30% glass fibre-reinforced grade RG-5030.

 

Applications

Radel® R-5100 is developed for injection moulding purposes.

Due to its high thermal stability, the Radel® R-5100 finds applications in medical equipment such as sterilisation cases and trays, as well as dental and surgical instruments. Its high hydrolytic stability also allows for it to be steam sterilised for over 1000 cycles without significantly losing its functional properties. It has also been cleared for safety for use in the human body and can be used as implantable devices. Its high chemical resistance notably includes chlorine, which is present in many disinfectants and detergents.

 

Fuentes

Quick statistics:

  • Density: 1.3 g/cm³
  • Impact strength, Izod notched: 690 J/m
  • Heat deflection temperature: 214 °C
  • Glass transition temperature: 220 °C
  • Elongation: 60 %
  • Tensile strength: 69.6 MPa


Click here for the full technical data sheet (TDS).