General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.3 g/cm³ Show Material materials with Densidad of 1.3 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.42 [-] Show Material materials with Coeficiente de Poisson of 0.42 [-] | ASTM E132 | ||
Elongación | 23.0 °C | 60 % Show Material materials with Elongación of 60 % | ASTM D638 | ||
Elongation at yield | 23.0 °C | 7.2 % Show Material materials with Elongation at yield of 7.2 % | ASTM D638 | ||
Flexural yield strength | 23.0 °C | 91 MPa Show Material materials with Flexural yield strength of 91 MPa | ASTM D790 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 690 J/m Show Material materials with Impact strength, Izod notched, ASTM of 690 J/m | ASTM D256 | ||
Límite elástico | 23.0 °C | 69.6 MPa Show Material materials with Límite elástico of 69.6 MPa | ASTM D638 | ||
Módulo de compresión | 23.0 °C | 1.73 MPa Show Material materials with Módulo de compresión of 1.73 MPa | ASTM D695 | ||
Módulo de flexión | 23.0 °C | 1.7 GPa Show Material materials with Módulo de flexión of 1.7 GPa | ASTM D790 | ||
Módulo elástico | 23.0 °C | 2.34 GPa Show Material materials with Módulo elástico of 2.34 GPa | ASTM D638 | ||
Resistencia a la compresión | 23.0 °C | 98.9 MPa Show Material materials with Resistencia a la compresión of 98.9 MPa | ASTM D695 | ||
Resistencia a la tracción | 23.0 °C | 69.6 MPa Show Material materials with Resistencia a la tracción of 69.6 MPa | ASTM D638 | ||
Resistencia al cizallamiento | 23.0 °C | 62.7 MPa Show Material materials with Resistencia al cizallamiento of 62.7 MPa | ASTM D732 | ||
Impact strength, Izod unnotched, ASTM | No Break, ASTM D256 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 5.6E-5 1/K | ASTM D696 | ||
Conductividad térmica | 23.0 °C | 0.35 W/(m·K) Show Material materials with Conductividad térmica of 0.35 W/(m·K) | ASTM C177 | ||
Heat deflection temperature, 0.45 MPa | 214 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 214 °C | ASTM D648 | |||
Temperatura de transición del vidrio | 220 °C Show Material materials with Temperatura de transición del vidrio of 220 °C | ASTM E1356 | |||
Inflamabilidad | V-0 UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.44 [-] Show Material materials with Constante dieléctrica of 3.44 [-] | ASTM D150, at 60 Hz |
Resistividad eléctrica | 23.0 °C | 9.00E+13 Ω·m Show Material materials with Resistividad eléctrica of 9.00E+13 Ω·m | |
Rigidez dieléctrica | 23.0 °C | 14 kV/mm Show Material materials with Rigidez dieléctrica of 14 kV/mm | ASTM D149 |
Óptico
Property | Value | Comment |
---|---|---|
Índice de refracción | 1.67 [-] Show Material materials with Índice de refracción of 1.67 [-] | ASTM D542 |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace Applications, Connectors,Dental Applications, Food Service Applications, Hospital Goods, Medical Devices,Medical/Healthcare Applications, Plumbing Parts,Surgical Instruments | |
Color | Transparent, Opaque, Black, Grey, Violet, Brown, Red, Yellow, Orange, Green, Violet | |
Processing methods | Blow Molding, Extrusion, Film Extrusion, Profile Extrusion, Sheet Extrusion, Thermoforming - Injection Molding: Drying Temperature: 149°C, Drying Time: 2.5 hr, Rear Temperature: 321°C, Middle Temperature: 349°C, Front Temperature: 349°C, Melt Temperature: 343-388°C, Mold Temperature: 138-163°C, Back Pressure: 0.345-0.689 MPa, Screw Compression Ratio: 2.2:1 |