Óxido de circonio
Zirconia fine ceramic Spray NozzleSuministrada por:
Zhengzhou Sky Universe Trade Co.,LtdOxide Based Ceramic Matrix Composite
Chemical Grade Yttria-Stabilized Zirconia RTP GNP3YGSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Chemical Grade Yttria-Stabilized Zirconia GNP3YSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Chemical Grade Yttria-Stabilized Zirconia RTP GNP3YG-BRSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Calcia-Stabilized Zirconia GNPPCK-aSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Calcia-Stabilized Zirconia PCDSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Calcia-Stabilized Zirconia PCD-CSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Calcia-Stabilized Zirconia FCDSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Yttria-Stabilized Zirconia GNP5YD-bSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Yttria-Stabilized Zirconia GNP7YD-aSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Yttria-Stabilized Zirconia GNP7YD-bSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Yttria-Stabilized Zirconia GNP7YD-aQSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Yttria-Stabilized Zirconia GNP7YD-cQSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Magnesia-Stabilized Zirconia GNPMD-aSuministrada por:
GNPGraystar Specialty MaterialsOxide Based Ceramic Matrix Composite
Fused Magnesia-Stabilized Zirconia GNPMD-bSuministrada por:
GNPGraystar Specialty Materials