General
Property | Value | Comment |
---|---|---|
Densidad | 2.6 - 2.7 g/cm³ Show Material materials with Densidad of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | ||
Dureza Brinell | 95.0 [-] Show Material materials with Dureza Brinell of 95.0 [-] | T61 | Pink Sheets, ASTM B955 | |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | ||
Resistencia a la tracción | 295.0 MPa Show Material materials with Resistencia a la tracción of 295.0 MPa | T61 | Pink Sheets, ASTM B955 |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium | ||
Coeficiente de dilatación térmica | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium | ||
Conductividad térmica | 60.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium | ||
Temperatura de fusión | 582.0 - 652.0 °C Show Material materials with Temperatura de fusión of 582.0 - 652.0 °C | T61 | Pink Sheets, ASTM B955 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 0.15 - 0.4 % Show Material materials with Cobre of 0.15 - 0.4 % | T61 | Pink Sheets, ASTM B955 |
Cromo | 0.04 - 0.35 % Show Material materials with Cromo of 0.04 - 0.35 % | T61 | Pink Sheets, ASTM B955 |
Hierro | 0.70 % Show Material materials with Hierro of 0.70 % | T61 | Pink Sheets, ASTM B955 |
Magnesio | 0.8 - 1.2 % Show Material materials with Magnesio of 0.8 - 1.2 % | T61 | Pink Sheets, ASTM B955 |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % | T61 | Pink Sheets, ASTM B955 |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % | T61 | Pink Sheets, ASTM B955 |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T61 | Pink Sheets, ASTM B955 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T61 | Pink Sheets, ASTM B955 |