General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Dureza Brinell | 18.0 [-] Show Material materials with Dureza Brinell of 18.0 [-] | F | EN 573-3, EN 570 | Strip, Sheet, Plate | |
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Resistencia a la tracción | 75.0 - 85.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 85.0 MPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
Coeficiente de dilatación térmica | -50 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
20 °C | 2.18e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.18e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
20 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
20 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
200 °C | 2.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.45e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
300 °C | 2.55e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.55e-05 1/K | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
Conductividad térmica | 232 W/(m·K) Show Material materials with Conductividad térmica of 232 W/(m·K) | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate | |
Temperatura de fusión | 660.0 °C Show Material materials with Temperatura de fusión of 660.0 °C | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 37500000.0 - 37700000.0 S/m Show Material materials with Conductividad eléctrica of 37500000.0 - 37700000.0 S/m | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Resistividad eléctrica | 2.65e-08 - 2.67e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.65e-08 - 2.67e-08 Ω·m | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.98 % Show Material materials with Aluminio of 99.98 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Cobre | 0.003 % Show Material materials with Cobre of 0.003 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Hierro | 0.006 % Show Material materials with Hierro of 0.006 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Titanio | 0.003 % Show Material materials with Titanio of 0.003 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Zinc | 0.015 % Show Material materials with Zinc of 0.015 % | F | EN 573-3, EN 1715-3, EN 570 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good, general: very good | |
Corrosion properties | Seawater: acceptable, weathering: good | |
Workability | Bending / Spinning (cold): very good |