General
Property | Value | Related Standards |
---|---|---|
Densidad | 2.82 g/cm³ Show Material materials with Densidad of 2.82 g/cm³ | AA Standards |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium |
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium |
Módulo elástico | 70.0 - 73.0 GPa Show Material materials with Módulo elástico of 70.0 - 73.0 GPa | Typical for Wrought 2000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 816.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 2000 Series Aluminium |
Conductividad térmica | 112.0 - 251.0 W/(m·K) Show Material materials with Conductividad térmica of 112.0 - 251.0 W/(m·K) | Typical for Wrought 2000 Series Aluminium |
Temperatura de fusión | 500.0 - 650.0 °C Show Material materials with Temperatura de fusión of 500.0 - 650.0 °C | Typical for Wrought 2000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Bismuto | 0.4 - 1.0 % Show Material materials with Bismuto of 0.4 - 1.0 % | AA Standards |
Cobre | 3.3 - 5.0 % Show Material materials with Cobre of 3.3 - 5.0 % | AA Standards |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | AA Standards |
Estaño | 0.2 - 1.0 % Show Material materials with Estaño of 0.2 - 1.0 % | AA Standards |
Hierro | 0.70 % Show Material materials with Hierro of 0.70 % | AA Standards |
Magnesio | 0.5 - 1.3 % Show Material materials with Magnesio of 0.5 - 1.3 % | AA Standards |
Manganeso | 0.2 - 1.0 % Show Material materials with Manganeso of 0.2 - 1.0 % | AA Standards |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % | AA Standards |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % | AA Standards |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | AA Standards |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | AA Standards |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |