General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.67 g/cm³ Show Material materials with Densidad of 2.67 g/cm³ | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
2.67 g/cm³ Show Material materials with Densidad of 2.67 g/cm³ | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | H18 | EN 573-3 | Rod, Flat, Tube, Wire |
Medidas
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 145.0 MPa Show Material materials with Bending Fatigue Strength of 145.0 MPa | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
Coeficiente de Poisson | 20.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | H18 | EN 573-3 | Rod, Flat, Tube, Wire | |
Dureza Brinell | 100.0 [-] Show Material materials with Dureza Brinell of 100.0 [-] | H18 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | ||
20.0 °C | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | H18 | EN 573-3 | Rod, Tube | ||
20.0 °C | 94.0 [-] Show Material materials with Dureza Brinell of 94.0 [-] | H18 | EN 573-3 | Flat | ||
Dureza Brinell (HBW) | 94 [-] Show Material materials with Dureza Brinell (HBW) of 94 [-] | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
Elongación | 1 % Show Material materials with Elongación of 1 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | A50 | |
1.0 % Show Material materials with Elongación of 1.0 % | H18 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
2.0 % Show Material materials with Elongación of 2.0 % | H18 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A50 | ||
2.0 % Show Material materials with Elongación of 2.0 % | H18 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
3.0 % Show Material materials with Elongación of 3.0 % | H18 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | A100 | ||
20.0 °C | 1.0 % Show Material materials with Elongación of 1.0 % | H18 | EN 573-3 | Flat | A50 | |
20.0 °C | 1.0 % Show Material materials with Elongación of 1.0 % | H18 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H18 | EN 573-3 | Rod, Tube | A50 | |
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H18 | EN 573-3 | Wire | A100 | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H18 | EN 573-3 | Rod, Tube | ||
Límite elástico | 240.0 MPa Show Material materials with Límite elástico of 240.0 MPa | H18 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | RP02 | |
270 MPa Show Material materials with Límite elástico of 270 MPa | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |||
285.0 MPa Show Material materials with Límite elástico of 285.0 MPa | H18 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | RP02 | ||
320.0 MPa Show Material materials with Límite elástico of 320.0 MPa | H18 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | RP02 | ||
20.0 °C | 240.0 MPa Show Material materials with Límite elástico of 240.0 MPa | H18 | EN 573-3 | Rod, Tube | RP02 | |
20.0 °C | 270.0 MPa Show Material materials with Límite elástico of 270.0 MPa | H18 | EN 573-3 | Flat | RP02 | |
20.0 °C | 270.0 MPa Show Material materials with Límite elástico of 270.0 MPa | H18 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 320.0 MPa Show Material materials with Límite elástico of 320.0 MPa | H18 | EN 573-3 | Wire | RP02 | |
Módulo de cizallamiento | 25.725 GPa Show Material materials with Módulo de cizallamiento of 25.725 GPa | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
26.6 GPa Show Material materials with Módulo de cizallamiento of 26.6 GPa | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
20.0 °C | 26.6 GPa Show Material materials with Módulo de cizallamiento of 26.6 GPa | H18 | EN 573-3 | Rod, Flat, Tube, Wire | ||
Módulo elástico | 68.6 GPa Show Material materials with Módulo elástico of 68.6 GPa | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
70.5 GPa Show Material materials with Módulo elástico of 70.5 GPa | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H18 | EN 573-3 | Rod, Flat, Tube, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
310.0 MPa Show Material materials with Resistencia a la tracción of 310.0 MPa | H18 | EN 573-3, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | H18 | EN 573-3, EN 1301, EN 485 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |||
20.0 °C | 310.0 MPa Show Material materials with Resistencia a la tracción of 310.0 MPa | H18 | EN 573-3 | Rod, Tube, Flat | ||
20.0 °C | 310.0 MPa Show Material materials with Resistencia a la tracción of 310.0 MPa | H18 | EN 573-3 | Flat | Transverse | |
20.0 °C | 330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | H18 | EN 573-3 | Wire |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 897.0 J/(kg·K) Show Material materials with Calor específico of 897.0 J/(kg·K) | H18 | EN 573-3 | Rod, Flat, Tube, Wire | |
Coeficiente de dilatación térmica | 100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | 20-100°C |
Conductividad térmica | 134 W/(m·K) Show Material materials with Conductividad térmica of 134 W/(m·K) | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
20.0 °C | 129.0 W/(m·K) Show Material materials with Conductividad térmica of 129.0 W/(m·K) | H18 | EN 573-3 | Rod, Flat, Tube, Wire | ||
Temperatura de fusión | 560.0 - 655.0 °C Show Material materials with Temperatura de fusión of 560.0 - 655.0 °C | Typical for Wrought 5000 Series Aluminium | ||||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 18000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium | ||||
Resistividad eléctrica | 5.2e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.2e-08 Ω·m | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | ||
20.0 °C | 5.4e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.4e-08 Ω·m | H18 | EN 573-3 | Rod, Flat, Tube, Wire |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.1 % Show Material materials with Cobre of 0.1 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.25 % Show Material materials with Cromo of 0.25 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | H18 | EN 573-3 | Rod, Flat, Tube, Wire |
0.5 % Show Material materials with Hierro of 0.5 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
0.50 % Show Material materials with Hierro of 0.50 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Strip, Sheet, Plate, Rod, Welded Tube, Tube, Wire | |
Magnesio | 3.1 - 3.9 % Show Material materials with Magnesio of 3.1 - 3.9 % | H18 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Coil, Sheet, Strip, Strip, Sheet, Plate, Welded Tube |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.5 % Show Material materials with Manganeso of 0.5 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Otro | 0.05 - 0.15 % Show Material materials with Otro of 0.05 - 0.15 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.5 % Show Material materials with Silicona of 0.5 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.2 % Show Material materials with Titanio of 0.2 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip | |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H18 | EN 573-3, EN 1301, EN 485, EN 754 | Rod, Flat, Tube, Wire, Strip, Sheet, Plate, Welded Tube |
0.2 % Show Material materials with Zinc of 0.2 % | H18 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Food can: Body, Lids | |
Brazing | hard brazing (with flux/ without flux): sufficient - not suitable / sufficient, friction soldering: acceptable, soft brazing with flux: poor | |
Corrosion properties | Excellent | |
General machinability | Good | |
Welding | Good | |
Workability | Good |