General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.65 g/cm³ Show Material materials with Densidad of 2.65 g/cm³ | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | |
2.65 g/cm³ Show Material materials with Densidad of 2.65 g/cm³ | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 2.64 g/cm³ Show Material materials with Densidad of 2.64 g/cm³ | H19 | EN 573-3 | Sheet, Flat |
Medidas
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||||
Dureza Brinell | 114.0 [-] Show Material materials with Dureza Brinell of 114.0 [-] | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 114.0 [-] Show Material materials with Dureza Brinell of 114.0 [-] | H19 | EN 573-3 | Flat | ||
Dureza Brinell (HBW) | 114 [-] Show Material materials with Dureza Brinell (HBW) of 114 [-] | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Límite elástico | 320.0 MPa Show Material materials with Límite elástico of 320.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | RP02 | |
320 MPa Show Material materials with Límite elástico of 320 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |||
20.0 °C | 310.0 - 390.0 MPa Show Material materials with Límite elástico of 310.0 - 390.0 MPa | H19 | EN 573-3 | Sheet | RP02 | |
20.0 °C | 310.0 - 340.0 MPa Show Material materials with Límite elástico of 310.0 - 340.0 MPa | H19 | EN 573-3 | Sheet | RP02 | |
20.0 °C | 320.0 MPa Show Material materials with Límite elástico of 320.0 MPa | H19 | EN 573-3 | Flat | RP02 | |
20.0 °C | 320.0 MPa Show Material materials with Límite elástico of 320.0 MPa | H19 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 330.0 - 390.0 MPa Show Material materials with Límite elástico of 330.0 - 390.0 MPa | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | RP02 | |
20.0 °C | 330.0 - 340.0 MPa Show Material materials with Límite elástico of 330.0 - 340.0 MPa | H19 | EN 573-3 | Sheet | RP02 | |
Módulo de cizallamiento | 20.0 °C | 27.0 GPa Show Material materials with Módulo de cizallamiento of 27.0 GPa | H19 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Sheet, Flat, Coil, Sheet | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | ||
71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | H19 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
380 MPa Show Material materials with Resistencia a la tracción of 380 MPa | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |||
20.0 °C | 350.0 - 430.0 MPa Show Material materials with Resistencia a la tracción of 350.0 - 430.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 350.0 - 390.0 MPa Show Material materials with Resistencia a la tracción of 350.0 - 390.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 370.0 - 430.0 MPa Show Material materials with Resistencia a la tracción of 370.0 - 430.0 MPa | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | ||
20.0 °C | 370.0 - 390.0 MPa Show Material materials with Resistencia a la tracción of 370.0 - 390.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | H19 | EN 573-3 | Flat | ||
20.0 °C | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | H19 | EN 573-3 | Flat | Transverse |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | H19 | EN 573-3 | Sheet, Flat | |
Coeficiente de dilatación térmica | 20 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | |
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | ||
100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | 20-100°C | |
Conductividad térmica | 121 W/(m·K) Show Material materials with Conductividad térmica of 121 W/(m·K) | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
123 W/(m·K) Show Material materials with Conductividad térmica of 123 W/(m·K) | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | |||
20.0 °C | 140.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 W/(m·K) | H19 | EN 573-3 | Sheet, Flat | ||
Temperatura de fusión | 577.0 - 638.0 °C Show Material materials with Temperatura de fusión of 577.0 - 638.0 °C | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | ||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 18000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 S/m | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | |
20.0 °C | 19000000.0 S/m Show Material materials with Conductividad eléctrica of 19000000.0 S/m | H19 | EN 573-3 | Sheet, Flat | |
Resistividad eléctrica | 5.56e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.56e-08 Ω·m | H19 | EN 573-3, EN 485, EN 541 | Strip, Sheet, Plate | |
5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.6e-08 Ω·m | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat, Strip, Plate |
0.15 % Show Material materials with Cobre of 0.15 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat, Strip, Plate |
0.1 % Show Material materials with Cromo of 0.1 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | H19 | EN 573-3 | Sheet, Flat |
0.35 % Show Material materials with Hierro of 0.35 % | H19 | EN 573-3, EN 485, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Strip, Sheet, Plate, Coil, Sheet | |
Magnesio | 4.0 - 5.0 % Show Material materials with Magnesio of 4.0 - 5.0 % | H19 | EN 573-3, EN 485, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Sheet, Flat, Strip, Plate, Coil, Sheet |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % | H19 | EN 573-3, EN 485, EN 541, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Sheet, Flat, Strip, Plate, Coil, Sheet |
Otro | 0.05 - 0.15 % Show Material materials with Otro of 0.05 - 0.15 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat, Strip, Plate |
0.2 % Show Material materials with Silicona of 0.2 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat, Strip, Plate |
0.1 % Show Material materials with Titanio of 0.1 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H19 | EN 573-3, EN 485, EN 541 | Sheet, Flat, Strip, Plate |
0.25 % Show Material materials with Zinc of 0.25 % | H19 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: good | |
Application areas | Wind energy: Nacelle coverings, rotor hub, stairs; Components: Heat shields, Access hatches, Spoilers, General tranportation | |
Brazing | hard brazing (with flux/ without flux): sufficient to not suitable / poor, friction soldering: acceptable, soft brazing with flux: poor | |
Corrosion properties | Seawater: very good, weathering: very good | |
Welding | Good | |
Workability | Bending / Spinning (cold): good / sufficient, Impact extrusion (cold): sufficient, Deep drawing / upsetting (Condition) good (O) / acceptable (O) |