General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | F | EN 573-3 | Profile, Rod, Flat, Tube | |
20.0 °C | 2.68 - 2.69 g/cm³ Show Material materials with Densidad of 2.68 - 2.69 g/cm³ | F | EN 573-3 | Profile, Rod, Flat, Tube | |
20.0 °C | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | F | EN 573-3 | Profile, Rod, Flat, Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | F | EN 573-3 | Profile, Rod, Flat, Tube | |
Dureza Brinell | 45.0 [-] Show Material materials with Dureza Brinell of 45.0 [-] | F | EN 573-3, EN 570 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 45.0 [-] Show Material materials with Dureza Brinell of 45.0 [-] | F | EN 573-3 | Profile, Rod, Tube | ||
Elongación | 14.0 % Show Material materials with Elongación of 14.0 % | F | EN 573-3, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A50 | |
16.0 % Show Material materials with Elongación of 16.0 % | F | EN 573-3, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A100 | ||
20.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | F | EN 573-3 | Profile, Rod, Tube | A50 | |
20.0 °C | 16.0 % Show Material materials with Elongación of 16.0 % | F | EN 573-3 | Profile, Rod, Tube | ||
Módulo de cizallamiento | 26.3 GPa Show Material materials with Módulo de cizallamiento of 26.3 GPa | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 26.3 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.3 - 26.5 GPa | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
20.0 °C | 26.3 GPa Show Material materials with Módulo de cizallamiento of 26.3 GPa | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | F | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
170.0 - 230.0 MPa Show Material materials with Resistencia a la tracción of 170.0 - 230.0 MPa | F | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
20.0 °C | 160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | F | EN 573-3 | Profile, Rod, Tube, Flat | ||
20.0 °C | 160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | F | EN 573-3 | Flat | Transverse |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 898.0 - 921.0 J/(kg·K) Show Material materials with Calor específico of 898.0 - 921.0 J/(kg·K) | F | EN 573-3 | Profile, Rod, Flat, Tube | |
20.0 °C | 898.0 J/(kg·K) Show Material materials with Calor específico of 898.0 J/(kg·K) | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
Coeficiente de dilatación térmica | 20 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
100 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
Conductividad térmica | 140.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 - 160.0 W/(m·K) | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 149.0 - 167.0 W/(m·K) Show Material materials with Conductividad térmica of 149.0 - 167.0 W/(m·K) | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
20.0 °C | 149.0 W/(m·K) Show Material materials with Conductividad térmica of 149.0 W/(m·K) | F | EN 573-3 | Profile, Rod, Flat, Tube | ||
Temperatura de fusión | 610.0 - 650.0 °C Show Material materials with Temperatura de fusión of 610.0 - 650.0 °C | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 25000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 25000000.0 - 30000000.0 S/m | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
20.0 °C | 26000000.0 S/m Show Material materials with Conductividad eléctrica of 26000000.0 S/m | F | EN 573-3 | Profile, Rod, Flat, Tube | |
Resistividad eléctrica | 3.33e-08 - 4e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.33e-08 - 4e-08 Ω·m | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
20.0 °C | 4.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.6e-08 Ω·m | F | EN 573-3 | Profile, Rod, Flat, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | F | EN 573-3 | Profile, Rod, Flat, Tube |
0.50 % Show Material materials with Hierro of 0.50 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
Magnesio | 1.7 - 2.4 % Show Material materials with Magnesio of 1.7 - 2.4 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Manganeso | 0.1 - 0.5 % Show Material materials with Manganeso of 0.1 - 0.5 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Zinc | 0.15 % Show Material materials with Zinc of 0.15 % | F | EN 573-3, EN 1715-3, EN 485, EN 570, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): sufficient / poor, friction soldering: good, soft brazing with flux: sufficient | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / acceptable (H12) |