General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
20.0 °C | 2.68 g/cm³ Show Material materials with Densidad of 2.68 g/cm³ | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | |
20.0 °C | 2.68 - 2.69 g/cm³ Show Material materials with Densidad of 2.68 - 2.69 g/cm³ | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | |
20.0 °C | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 573-3 | Coil, Sheet, Plate, Strip, Rod, Flat, Seamless Tube, Tube, Wire |
Medidas
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Espesor | 0.2 mm Show Material materials with Espesor of 0.2 mm | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | 0.2 mm | Coil, Sheet, Plate, Strip |
6.0 mm Show Material materials with Espesor of 6.0 mm | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | 6.0 mm | Coil, Sheet, Plate, Strip |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 115.0 MPa Show Material materials with Bending Fatigue Strength of 115.0 MPa | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
Coeficiente de Poisson | 20.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | |
Dureza Brinell | 64.0 [-] Show Material materials with Dureza Brinell of 64.0 [-] | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 64.0 [-] Show Material materials with Dureza Brinell of 64.0 [-] | H14 | EN 573-3 | Flat | ||
20.0 °C | 65.0 [-] Show Material materials with Dureza Brinell of 65.0 [-] | H14 | EN 573-3 | Rod, Tube | ||
Dureza Brinell (HBW) | 64 [-] Show Material materials with Dureza Brinell (HBW) of 64 [-] | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | ||
Elongación | 2.0 % Show Material materials with Elongación of 2.0 % | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A50 | |
2.0 - 4.0 % Show Material materials with Elongación of 2.0 - 4.0 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | A50 | ||
3.0 % Show Material materials with Elongación of 3.0 % | H14 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A50 | ||
4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A50 | ||
4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A100 | ||
5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A50 | ||
5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A100 | ||
6.0 % Show Material materials with Elongación of 6.0 % | H14 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | A100 | ||
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H14 | EN 573-3 | Flat | A50 | |
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | H14 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H14 | EN 573-3 | Tube, Flat | A50 | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H14 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3 | Rod, Flat | A50 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3 | Tube | ||
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H14 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3 | Flat | A50 | |
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3 | Rod | ||
20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | H14 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | H14 | EN 573-3 | Seamless Tube | ||
Límite elástico | 160.0 MPa Show Material materials with Límite elástico of 160.0 MPa | H14 | EN 573-3, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | RP02 | |
170.0 MPa Show Material materials with Límite elástico of 170.0 MPa | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | RP02 | ||
170 MPa Show Material materials with Límite elástico of 170 MPa | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |||
190.0 MPa Show Material materials with Límite elástico of 190.0 MPa | H14 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | RP02 | ||
220.0 MPa Show Material materials with Límite elástico of 220.0 MPa | H14 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | RP02 | ||
20.0 °C | 160.0 MPa Show Material materials with Límite elástico of 160.0 MPa | H14 | EN 573-3 | Rod, Tube | RP02 | |
20.0 °C | 170.0 MPa Show Material materials with Límite elástico of 170.0 MPa | H14 | EN 573-3 | Flat | RP02 | |
20.0 °C | 170.0 MPa Show Material materials with Límite elástico of 170.0 MPa | H14 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 190.0 MPa Show Material materials with Límite elástico of 190.0 MPa | H14 | EN 573-3 | Seamless Tube | RP02 | |
Módulo de cizallamiento | 26.3 GPa Show Material materials with Módulo de cizallamiento of 26.3 GPa | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
20.0 °C | 26.3 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.3 - 26.5 GPa | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
20.0 °C | 26.3 GPa Show Material materials with Módulo de cizallamiento of 26.3 GPa | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
Módulo elástico | 68.6 GPa Show Material materials with Módulo elástico of 68.6 GPa | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
20.0 °C | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||||
Resistencia a la tracción | 215.0 - 265.0 MPa Show Material materials with Resistencia a la tracción of 215.0 - 265.0 MPa | H14 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
230.0 MPa Show Material materials with Resistencia a la tracción of 230.0 MPa | H14 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
20.0 °C | 200.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 200.0 - 240.0 MPa | H14 | EN 573-3, EN 754 | Rod, Tube, Strip, Sheet, Plate, Wire, Welded Tube, Bar | ||
20.0 °C | 210.0 - 250.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 250.0 MPa | H14 | EN 573-3, EN 485, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Flat, Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar, Coil, Sheet, Plate, Strip | ||
20.0 °C | 210.0 - 250.0 MPa Show Material materials with Resistencia a la tracción of 210.0 - 250.0 MPa | H14 | EN 573-3 | Flat | Transverse | |
20.0 °C | 230.0 MPa Show Material materials with Resistencia a la tracción of 230.0 MPa | H14 | EN 573-3 | Seamless Tube | ||
Ángulo de flexión a 180° | 2.5 °/t Show Material materials with Ángulo de flexión a 180° of 2.5 °/t | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
2.5 °/t Show Material materials with Ángulo de flexión a 180° of 2.5 °/t | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |||
Ángulo de flexión a 90° | 0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |||
1.5 °/t Show Material materials with Ángulo de flexión a 90° of 1.5 °/t | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
2.5 °/t Show Material materials with Ángulo de flexión a 90° of 2.5 °/t | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |||
2.5 °/t Show Material materials with Ángulo de flexión a 90° of 2.5 °/t | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |||
3.0 °/t Show Material materials with Ángulo de flexión a 90° of 3.0 °/t | H14 | EN 573-3, EN 485 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 898.0 - 921.0 J/(kg·K) Show Material materials with Calor específico of 898.0 - 921.0 J/(kg·K) | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | |
20.0 °C | 898.0 J/(kg·K) Show Material materials with Calor específico of 898.0 J/(kg·K) | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
Coeficiente de dilatación térmica | 20 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
100 °C | 2.3699999999999997e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3699999999999997e-05 1/K | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | 20-100°C | |
Conductividad térmica | 140.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 - 160.0 W/(m·K) | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
153 W/(m·K) Show Material materials with Conductividad térmica of 153 W/(m·K) | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |||
20.0 °C | 149.0 - 167.0 W/(m·K) Show Material materials with Conductividad térmica of 149.0 - 167.0 W/(m·K) | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
20.0 °C | 149.0 W/(m·K) Show Material materials with Conductividad térmica of 149.0 W/(m·K) | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | ||
Temperatura de fusión | 610.0 - 650.0 °C Show Material materials with Temperatura de fusión of 610.0 - 650.0 °C | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | ||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 25000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 25000000.0 - 30000000.0 S/m | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
20.0 °C | 26000000.0 S/m Show Material materials with Conductividad eléctrica of 26000000.0 S/m | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire | |
Resistividad eléctrica | 3.33e-08 - 4e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.33e-08 - 4e-08 Ω·m | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
4.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.5e-08 Ω·m | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | ||
20.0 °C | 4.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.6e-08 Ω·m | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar |
0.15 % Show Material materials with Cobre of 0.15 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar |
0.15 % Show Material materials with Cromo of 0.15 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | H14 | EN 573-3 | Rod, Flat, Seamless Tube, Tube, Wire |
0.50 % Show Material materials with Hierro of 0.50 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Strip, Sheet, Plate, Wire, Tube, Welded Tube, Bar | |
0.5 % Show Material materials with Hierro of 0.5 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |
Magnesio | 1.7 - 2.4 % Show Material materials with Magnesio of 1.7 - 2.4 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar, Coil, Sheet, Plate, Strip |
Manganeso | 0.1 - 0.5 % Show Material materials with Manganeso of 0.1 - 0.5 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754, EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar, Coil, Sheet, Plate, Strip |
Otro | 0.05 - 0.15 % Show Material materials with Otro of 0.05 - 0.15 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar |
0.4 % Show Material materials with Silicona of 0.4 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar |
0.15 % Show Material materials with Titanio of 0.15 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip | |
Zinc | 0.15 % Show Material materials with Zinc of 0.15 % | H14 | EN 573-3, EN 1301, EN 1592, EN 485, EN 754 | Rod, Flat, Seamless Tube, Tube, Wire, Strip, Sheet, Plate, Welded Tube, Bar |
0.15 % Show Material materials with Zinc of 0.15 % | H14 | EN 573-1, EN 573-2, EN 573-3, EN 485-2 | Coil, Sheet, Plate, Strip |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Tubes: Industrial tubes, Pipes; Wind energy: Nacelle coverings, rotor hub, stairs; | |
Brazing | hard brazing (with flux/ without flux): sufficient / poor, friction soldering: good, soft brazing with flux: sufficient | |
Corrosion properties | Seawater: good, weathering: very good | |
Welding | Very Good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) good (O) / acceptable (H12) |