General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 2.66 g/cm³ Show Material materials with Densidad of 2.66 g/cm³ | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||
Resistencia a la tracción | 265.0 MPa Show Material materials with Resistencia a la tracción of 265.0 MPa | O | AA Standards, ASTM B209 | |
270.0 MPa Show Material materials with Resistencia a la tracción of 270.0 MPa | O | AA Standards, ASTM B209 | ||
275.0 MPa Show Material materials with Resistencia a la tracción of 275.0 MPa | O | AA Standards, ASTM B209 | ||
285.0 - 360.0 MPa Show Material materials with Resistencia a la tracción of 285.0 - 360.0 MPa | O | AA Standards, ASTM B209 | ||
285.0 - 365.0 MPa Show Material materials with Resistencia a la tracción of 285.0 - 365.0 MPa | O | AA Standards, ASTM B210, ASTM B221, ASTM B241 | ||
290.0 - 365.0 MPa Show Material materials with Resistencia a la tracción of 290.0 - 365.0 MPa | O | AA Standards, ASTM B209 | ||
310.0 MPa Show Material materials with Resistencia a la tracción of 310.0 MPa | O | AA Standards |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 879.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | |||
Coeficiente de dilatación térmica | 20 °C | 2.3899999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3899999999999998e-05 1/K | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 | |
100 °C | 2.3899999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3899999999999998e-05 1/K | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 | ||
Conductividad térmica | 117.0 Show Material materials with Conductividad térmica of 117.0 | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 | ||
Temperatura de fusión | 570.0 - 640.0 °C Show Material materials with Temperatura de fusión of 570.0 - 640.0 °C | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 | ||
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 17000000.0 S/m Show Material materials with Conductividad eléctrica of 17000000.0 S/m | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Resistividad eléctrica | 5.88e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.88e-08 Ω·m | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Cromo | 0.05 - 0.2 % Show Material materials with Cromo of 0.05 - 0.2 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Magnesio | 4.7 - 5.5 % Show Material materials with Magnesio of 4.7 - 5.5 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Manganeso | 0.5 - 1.0 % Show Material materials with Manganeso of 0.5 - 1.0 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | O | AA Standards, ASTM B209, ASTM B210, ASTM B221, ASTM B241 |
Technological properties
Property | ||
---|---|---|
Brazing | general: no brazing is known or developed | |
Corrosion properties | Stress corrosion cracking: no damage during operation, limited damage during laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (O, H321, H116) | |
Workability | general (condition): acceptable (O), poor(H321, H116) |