General
Property | Value | Related Standards |
---|---|---|
Densidad | 2.84 g/cm³ Show Material materials with Densidad of 2.84 g/cm³ | AA Standards |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium |
Módulo de cizallamiento | 26.4 - 27.1 GPa Show Material materials with Módulo de cizallamiento of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium |
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Conductividad térmica | 121.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Circonio | 0.11 - 0.2 % Show Material materials with Circonio of 0.11 - 0.2 % | AA Standards |
Cobre | 1.3 - 1.9 % Show Material materials with Cobre of 1.3 - 1.9 % | AA Standards |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | AA Standards |
Escandio | 0.18 - 0.5 % Show Material materials with Escandio of 0.18 - 0.5 % | AA Standards |
Hierro | 0.20 % Show Material materials with Hierro of 0.20 % | AA Standards |
Magnesio | 2.0 - 2.8 % Show Material materials with Magnesio of 2.0 - 2.8 % | AA Standards |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % | AA Standards |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | AA Standards |
Zinc | 6.5 - 7.9 % Show Material materials with Zinc of 6.5 - 7.9 % | AA Standards |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |