General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
2.705 g/cm³ Show Material materials with Densidad of 2.705 g/cm³ | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Elongación | 23.0 % Show Material materials with Elongación of 23.0 % | F | EN 573-3, EN 755 | Plate, Rod | A50 | |
25.0 % Show Material materials with Elongación of 25.0 % | F | EN 573-3, EN 755 | Plate, Rod | A100 | ||
20.0 °C | 23.0 % Show Material materials with Elongación of 23.0 % | F | EN 573-3 | Profile, Rod, Tube | A50 | |
20.0 °C | 25.0 % Show Material materials with Elongación of 25.0 % | F | EN 573-3 | Profile, Rod, Tube | ||
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | ||||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Resistencia a la tracción | 60.0 MPa Show Material materials with Resistencia a la tracción of 60.0 MPa | F | EN 573-3, EN 485, EN 755 | Plate, Rod | ||
65.0 MPa Show Material materials with Resistencia a la tracción of 65.0 MPa | F | EN 573-3, EN 14121 | Plate, Rod | |||
20.0 °C | 60.0 MPa Show Material materials with Resistencia a la tracción of 60.0 MPa | F | EN 573-3 | Profile, Rod, Tube |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 900.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | |
20 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
100 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
100 °C | 2.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.38e-05 1/K | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
Conductividad térmica | 225.0 - 235.0 W/(m·K) Show Material materials with Conductividad térmica of 225.0 - 235.0 W/(m·K) | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
234 W/(m·K) Show Material materials with Conductividad térmica of 234 W/(m·K) | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | |||
Temperatura de fusión | 645.0 - 657.0 °C Show Material materials with Temperatura de fusión of 645.0 - 657.0 °C | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | ||
645.0 - 655.0 °C Show Material materials with Temperatura de fusión of 645.0 - 655.0 °C | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 35400000.0 - 36500000.0 S/m Show Material materials with Conductividad eléctrica of 35400000.0 - 36500000.0 S/m | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
36000000.0 S/m Show Material materials with Conductividad eléctrica of 36000000.0 S/m | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod | |
Resistividad eléctrica | 2.74e-08 - 2.82e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.74e-08 - 2.82e-08 Ω·m | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
2.78e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.78e-08 Ω·m | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 99.5 % Show Material materials with Aluminio of 99.5 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
Boro | 0.05 % Show Material materials with Boro of 0.05 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Cromo | 0.01 % Show Material materials with Cromo of 0.01 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Galio | 0.03 % Show Material materials with Galio of 0.03 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod |
0.4 % Show Material materials with Hierro of 0.4 % | F | EN 573-3 | Profile, Rod, Tube | |
Manganeso | 0.01 % Show Material materials with Manganeso of 0.01 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | F | EN 573-3, EN 14121, EN 485, EN 755 | Plate, Rod, Profile, Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |