General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.78 g/cm³ Show Material materials with Densidad of 2.78 g/cm³ | T6 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | ||||
Dureza Brinell | 120.0 [-] Show Material materials with Dureza Brinell of 120.0 [-] | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | ||
121.0 [-] Show Material materials with Dureza Brinell of 121.0 [-] | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | |||
20.0 °C | 120.0 [-] Show Material materials with Dureza Brinell of 120.0 [-] | T6 | EN 573-3 | Profile, Rod, Tube | ||
20.0 °C | 121.0 [-] Show Material materials with Dureza Brinell of 121.0 [-] | T6 | EN 573-3 | Flat | ||
Elongación | 7.0 % Show Material materials with Elongación of 7.0 % | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | A50 | |
8.0 % Show Material materials with Elongación of 8.0 % | T6 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | A50 | ||
10.0 % Show Material materials with Elongación of 10.0 % | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | A100 | ||
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T6 | EN 573-3 | Flat | A50 | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T6 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T6 | EN 573-3 | Profile, Rod, Tube, Flat | A50 | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T6 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T6 | EN 573-3 | Profile, Rod, Tube | ||
Módulo de cizallamiento | 26.4 - 27.1 GPa Show Material materials with Módulo de cizallamiento of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 7000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | ||||
Resistencia a la tracción | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T6 | EN 573-3, EN 485 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | ||
410.0 MPa Show Material materials with Resistencia a la tracción of 410.0 MPa | T6 | EN 573-3, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | |||
20.0 °C | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T6 | EN 573-3 | Flat | ||
20.0 °C | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T6 | EN 573-3 | Flat | Transverse | |
20.0 °C | 410.0 MPa Show Material materials with Resistencia a la tracción of 410.0 MPa | T6 | EN 573-3 | Profile, Rod, Tube |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 795.0 - 1050.0 J/(kg·K) Show Material materials with Calor específico of 795.0 - 1050.0 J/(kg·K) | Typical for Wrought 7000 Series Aluminium |
Coeficiente de dilatación térmica | 2.1e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 - 2.4e-05 1/K | Typical for Wrought 7000 Series Aluminium |
Conductividad térmica | 121.0 - 170.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 170.0 W/(m·K) | Typical for Wrought 7000 Series Aluminium |
Temperatura de fusión | 465.0 - 655.0 °C Show Material materials with Temperatura de fusión of 465.0 - 655.0 °C | Typical for Wrought 7000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Circonio | 0.08 - 0.18 % Show Material materials with Circonio of 0.08 - 0.18 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | T6 | EN 573-3 | Profile, Rod, Flat, Tube |
0.40 % Show Material materials with Hierro of 0.40 % | T6 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Rod, Tube, Welded Tube | |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Zinc | 5.0 - 6.0 % Show Material materials with Zinc of 5.0 - 6.0 % | T6 | EN 573-3, EN 485, EN 755 | Profile, Rod, Flat, Tube, Strip, Sheet, Plate, Welded Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |