Mecánica
Property | Temperature | Value |
---|---|---|
Resistencia a la tracción | 20.0 °C | 160 - 200 MPa Show Material materials with Resistencia a la tracción of 160 - 200 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 99.5 % Show Material materials with Aluminio of 99.5 % |
Boro | 0.05 % Show Material materials with Boro of 0.05 % |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % |
Cromo | 0.01 % Show Material materials with Cromo of 0.01 % |
Galio | 0.03 % Show Material materials with Galio of 0.03 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Manganeso | 0.01 % Show Material materials with Manganeso of 0.01 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |