General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.82 g/cm³ Show Material materials with Densidad of 2.82 g/cm³ | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
2.83 g/cm³ Show Material materials with Densidad of 2.83 g/cm³ | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Módulo de cizallamiento | 27.3 GPa Show Material materials with Módulo de cizallamiento of 27.3 GPa | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
72.5 GPa Show Material materials with Módulo elástico of 72.5 GPa | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Resistencia a la tracción | 110.0 - 170.0 MPa Show Material materials with Resistencia a la tracción of 110.0 - 170.0 MPa | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 864.0 J/(kg·K) Show Material materials with Calor específico of 864.0 J/(kg·K) | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Coeficiente de dilatación térmica | -50 °C | 2.14e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.14e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
20 °C | 2.14e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.14e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
20 °C | 2.2899999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2899999999999998e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
20 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
20 °C | 2.4999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4999999999999998e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.2899999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2899999999999998e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
200 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
300 °C | 2.4999999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4999999999999998e-05 1/K | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Conductividad térmica | 151.0 - 172.0 W/(m·K) Show Material materials with Conductividad térmica of 151.0 - 172.0 W/(m·K) | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
170.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 170.0 - 220.0 W/(m·K) | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | ||
Temperatura de fusión | 540.0 - 645.0 °C Show Material materials with Temperatura de fusión of 540.0 - 645.0 °C | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
585.0 - 650.0 °C Show Material materials with Temperatura de fusión of 585.0 - 650.0 °C | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 23000000.0 - 26000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 26000000.0 S/m | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
24000000.0 - 32000000.0 S/m Show Material materials with Conductividad eléctrica of 24000000.0 - 32000000.0 S/m | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar | |
Resistividad eléctrica | 3.13e-08 - 4.17e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.13e-08 - 4.17e-08 Ω·m | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
3.85e-08 - 4.35e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.85e-08 - 4.35e-08 Ω·m | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bismuto | 0.2 - 0.6 % Show Material materials with Bismuto of 0.2 - 0.6 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Cobre | 5.0 - 6.0 % Show Material materials with Cobre of 5.0 - 6.0 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Hierro | 0.70 % Show Material materials with Hierro of 0.70 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Plomo | 0.2 - 0.6 % Show Material materials with Plomo of 0.2 - 0.6 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | O3 | EN 573-3, EN 1715-3 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: poor | |
Brazing | hard brazing (with flux/ without flux): not suitable /, friction soldering: sufficient | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Deep drawing / upsetting (Condition) - / acceptable |