General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | ||
Dureza Brinell | 150.0 [-] Show Material materials with Dureza Brinell of 150.0 [-] | T61 | Pink Sheets, ASTM B955 | |
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | ||
Resistencia a la tracción | 510.0 MPa Show Material materials with Resistencia a la tracción of 510.0 MPa | T61 | Pink Sheets, ASTM B955 |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | ||
Coeficiente de dilatación térmica | 2.4e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium | ||
Conductividad térmica | 100.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium | ||
Temperatura de fusión | 477.0 - 635.0 °C Show Material materials with Temperatura de fusión of 477.0 - 635.0 °C | T61 | Pink Sheets, ASTM B955 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 1.2 - 2.0 % Show Material materials with Cobre of 1.2 - 2.0 % | T61 | Pink Sheets, ASTM B955 |
Cromo | 0.18 - 0.28 % Show Material materials with Cromo of 0.18 - 0.28 % | T61 | Pink Sheets, ASTM B955 |
Hierro | 0.50 % Show Material materials with Hierro of 0.50 % | T61 | Pink Sheets, ASTM B955 |
Magnesio | 2.1 - 2.9 % Show Material materials with Magnesio of 2.1 - 2.9 % | T61 | Pink Sheets, ASTM B955 |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % | T61 | Pink Sheets, ASTM B955 |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | T61 | Pink Sheets, ASTM B955 |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | T61 | Pink Sheets, ASTM B955 |
Zinc | 5.1 - 6.1 % Show Material materials with Zinc of 5.1 - 6.1 % | T61 | Pink Sheets, ASTM B955 |