EN 1706 Grade AC-71000 T1

Want to keep this datasheet? Save it now in your required format

Description

Material EN AC-AlZn5Mg is produced as sand and die cast. It shows the following casting characteristics and properties: plasticity: acceptable heat crack resistance: insufficient pressure tightness: insufficient workability (after heat-treatment): excellent worability (casting condition): excellent corrosion resistance: good decorative anodic oxidation: good weldability: acceptable polishability: good strength at room temperature: acceptable strength at increased temp. (up to 200°C): insufficient ductility (impact strength): good fatigue strength amounts 60 to 90 N/mm² ( best available casting method, values for vibration durability up to 50*10 hoch 6 cycles [Woehler diagram]).

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM,AluKey.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueComment

Densidad

2.8 g/cm³

Show Material materials with Densidad of 2.8 g/cm³

Typical for Cast 7xx.x Series Aluminium

Mecánica

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

60.0 - 90.0 MPa

Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa

T1

EN 1706

Casting

Coeficiente de Poisson

0.33 [-]

Show Material materials with Coeficiente de Poisson of 0.33 [-]

Typical for Cast 7xx.x Series Aluminium

Dureza Brinell

60.0 [-]

Show Material materials with Dureza Brinell of 60.0 [-]

T1

EN 1706

Casting

65.0 [-]

Show Material materials with Dureza Brinell of 65.0 [-]

T1

EN 1706

Casting

20.0 °C

60.0 [-]

Show Material materials with Dureza Brinell of 60.0 [-]

T1

EN 1706

20.0 °C

65.0 [-]

Show Material materials with Dureza Brinell of 65.0 [-]

T1

EN 1706

Módulo elástico

74.0 GPa

Show Material materials with Módulo elástico of 74.0 GPa

Typical for Cast 7xx.x Series Aluminium

Resistencia a la tracción

190.0 MPa

Show Material materials with Resistencia a la tracción of 190.0 MPa

T1

EN 1706

Casting

210.0 MPa

Show Material materials with Resistencia a la tracción of 210.0 MPa

T1

EN 1706

Casting

20.0 °C

190.0 MPa

Show Material materials with Resistencia a la tracción of 190.0 MPa

T1

EN 1706

20.0 °C

210.0 MPa

Show Material materials with Resistencia a la tracción of 210.0 MPa

T1

EN 1706

Aplicaciones térmicas

PropertyTemperatureValueConditionRelated StandardsShapeComment

Calor específico

963.0 J/(kg·K)

Show Material materials with Calor específico of 963.0 J/(kg·K)

Typical for Cast 7xx.x Series Aluminium

Coeficiente de dilatación térmica

20 °C

2.4e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K

T1

EN 1706

Casting

100.0 °C

2.4e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K

T1

EN 1706

Casting

100 °C

2.4e-05 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K

T1

EN 1706

Casting

Conductividad térmica

20.0 °C

130.0 - 140.0 W/(m·K)

Show Material materials with Conductividad térmica of 130.0 - 140.0 W/(m·K)

T1

EN 1706

Casting

Temperatura de fusión

550.0 - 645.0 °C

Show Material materials with Temperatura de fusión of 550.0 - 645.0 °C

Typical for Cast 7xx.x Series Aluminium

Eléctrico

PropertyTemperatureValueConditionRelated StandardsShape

Conductividad eléctrica

20.0 °C

19000000.0 - 21000000.0 S/m

Show Material materials with Conductividad eléctrica of 19000000.0 - 21000000.0 S/m

T1

EN 1706

Casting

Resistividad eléctrica

4.76e-08 - 5.26e-08 Ω·m

Show Material materials with Resistividad eléctrica of 4.76e-08 - 5.26e-08 Ω·m

T1

EN 1706

Casting

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminio

90.3 %

Show Material materials with Aluminio of 90.3 %

T1

EN 1706

Cobre

0.15 - 0.35 %

Show Material materials with Cobre of 0.15 - 0.35 %

T1

EN 1706

Casting

Cromo

0.15 - 0.6 %

Show Material materials with Cromo of 0.15 - 0.6 %

T1

EN 1706

Casting

Estaño

0.05 %

Show Material materials with Estaño of 0.05 %

T1

EN 1706

Casting

Hierro

0.8 %

Show Material materials with Hierro of 0.8 %

T1

EN 1706

0.80 %

Show Material materials with Hierro of 0.80 %

T1

EN 1706

Casting

Magnesio

0.4 - 0.7 %

Show Material materials with Magnesio of 0.4 - 0.7 %

T1

EN 1706

Casting

Manganeso

0.4 %

Show Material materials with Manganeso of 0.4 %

T1

EN 1706

Casting

Níquel

0.05 %

Show Material materials with Níquel of 0.05 %

T1

EN 1706

Casting

Plomo

0.05 %

Show Material materials with Plomo of 0.05 %

T1

EN 1706

Casting

Silicona

0.3 %

Show Material materials with Silicona of 0.3 %

T1

EN 1706

Casting

Titanio

0.1 - 0.25 %

Show Material materials with Titanio of 0.1 - 0.25 %

T1

EN 1706

Casting

Zinc

4.5 - 6.0 %

Show Material materials with Zinc of 4.5 - 6.0 %

T1

EN 1706

Casting

Technological properties

Property
Anodizing

decorative: good

Corrosion properties

general: good

General machinability

after thermal treatment: excellent, as cast: excellent

Processing methods

permanent mould casting, separately cast test sample