General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T1 | EN 1706 | Casting | |
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Dureza Brinell | 90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T1 | EN 1706 | Casting | |
100.0 [-] Show Material materials with Dureza Brinell of 100.0 [-] | T1 | EN 1706 | Casting | ||
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Resistencia a la tracción | 210.0 MPa Show Material materials with Resistencia a la tracción of 210.0 MPa | T1 | EN 1706 | Casting | |
260.0 MPa Show Material materials with Resistencia a la tracción of 260.0 MPa | T1 | EN 1706 | Casting |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T1 | EN 1706 | Casting | |
100 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T1 | EN 1706 | Casting | ||
Conductividad térmica | 120.0 - 130.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 130.0 W/(m·K) | T1 | EN 1706 | Casting | ||
Temperatura de fusión | 550.0 - 645.0 °C Show Material materials with Temperatura de fusión of 550.0 - 645.0 °C | Typical for Cast 7xx.x Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 17000000.0 - 20000000.0 S/m Show Material materials with Conductividad eléctrica of 17000000.0 - 20000000.0 S/m | T1 | EN 1706 | Casting |
Resistividad eléctrica | 5e-08 - 5.88e-08 Ω·m Show Material materials with Resistividad eléctrica of 5e-08 - 5.88e-08 Ω·m | T1 | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 78.8 % Show Material materials with Aluminio of 78.8 % | T1 | EN 1706 | |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T1 | EN 1706 | Casting |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % | T1 | EN 1706 | |
0.30 % Show Material materials with Hierro of 0.30 % | T1 | EN 1706 | Casting | |
Magnesio | 0.2 - 0.5 % Show Material materials with Magnesio of 0.2 - 0.5 % | T1 | EN 1706 | Casting |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % | T1 | EN 1706 | Casting |
Silicona | 7.5 - 9.5 % Show Material materials with Silicona of 7.5 - 9.5 % | T1 | EN 1706 | Casting |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T1 | EN 1706 | Casting |
Zinc | 9.0 - 10.5 % Show Material materials with Zinc of 9.0 - 10.5 % | T1 | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: acceptable | |
General machinability | as cast: excellent | |
Processing methods | permanent mould casting, separately cast test sample |