General
Property | Value | Comment |
---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Dureza Brinell | 75.0 [-] Show Material materials with Dureza Brinell of 75.0 [-] | T5 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Resistencia a la tracción | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 2.4e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium | |||
Conductividad térmica | 100.0 - 160.0 W/(m·K) Show Material materials with Conductividad térmica of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium | |||
Temperatura de fusión | 593.0 - 641.0 °C Show Material materials with Temperatura de fusión of 593.0 - 641.0 °C | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.4 - 1.0 % Show Material materials with Cobre of 0.4 - 1.0 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Cromo | 0.35 % Show Material materials with Cromo of 0.35 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Hierro | 1.10 % Show Material materials with Hierro of 1.10 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Magnesio | 0.2 - 0.5 % Show Material materials with Magnesio of 0.2 - 0.5 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Níquel | 0.15 % Show Material materials with Níquel of 0.15 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zinc | 7.0 - 8.0 % Show Material materials with Zinc of 7.0 - 8.0 % | T5 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |