General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil | |
20.0 °C | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | O | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Sheet, Strip, Foil, Flat, Coil, Sheet, Strip, Foil |
Medidas
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Espesor | 0.08 mm Show Material materials with Espesor of 0.08 mm | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | 0.08 mm | Coil, Sheet, Strip, Foil |
0.2 mm Show Material materials with Espesor of 0.2 mm | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | 0.2 mm | Coil, Sheet, Strip, Foil |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Dureza Brinell | 25.0 [-] Show Material materials with Dureza Brinell of 25.0 [-] | O | EN 573-3, EN 485 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 25.0 [-] Show Material materials with Dureza Brinell of 25.0 [-] | O | EN 573-3 | Flat | ||
Límite elástico | 30.0 MPa Show Material materials with Límite elástico of 30.0 MPa | O | EN 573-3, EN 1396, EN 485 | Strip, Sheet, Plate, Foil | RP02 | |
30.0 - 70.0 MPa Show Material materials with Límite elástico of 30.0 - 70.0 MPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | according to EN 485-2 | ||
70.0 MPa Show Material materials with Límite elástico of 70.0 MPa | O | EN 573-3, EN 683 | Strip, Sheet, Plate, Foil | RP02 | ||
20.0 °C | 30.0 MPa Show Material materials with Límite elástico of 30.0 MPa | O | EN 573-3 | Sheet, Strip, Flat | RP02 Transverse | |
20.0 °C | 30.0 MPa Show Material materials with Límite elástico of 30.0 MPa | O | EN 573-3 | Sheet, Strip, Flat | RP02 | |
20.0 °C | 70.0 MPa Show Material materials with Límite elástico of 70.0 MPa | O | EN 573-3 | Foil | RP02 | |
Módulo de cizallamiento | 25.725 GPa Show Material materials with Módulo de cizallamiento of 25.725 GPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | ||
Módulo elástico | 68.6 GPa Show Material materials with Módulo elástico of 68.6 GPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Resistencia a la tracción | 85.0 MPa Show Material materials with Resistencia a la tracción of 85.0 MPa | O | EN 573-3, EN 485 | Strip, Sheet, Plate, Foil | ||
90.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 90.0 - 120.0 MPa | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | according to EN 485-2 | ||
20.0 °C | 50.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 50.0 - 110.0 MPa | O | EN 573-3, EN 546 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 50.0 - 115.0 MPa Show Material materials with Resistencia a la tracción of 50.0 - 115.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 50.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 50.0 - 120.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 50.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 50.0 - 130.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 55.0 - 115.0 MPa Show Material materials with Resistencia a la tracción of 55.0 - 115.0 MPa | O | EN 573-3, EN 546 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 55.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 55.0 - 120.0 MPa | O | EN 573-3, EN 546 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 55.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 55.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 55.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 55.0 - 130.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 130.0 MPa | O | EN 573-3, EN 546, EN 683 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 65.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 115.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 115.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 120.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 80.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 120.0 MPa | O | EN 573-3 | Sheet, Strip | Transverse | |
20.0 °C | 80.0 - 120.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 120.0 MPa | O | EN 573-3, EN 1396 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 85.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 85.0 - 130.0 MPa | O | EN 573-3 | Flat | Transverse | |
20.0 °C | 85.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 85.0 - 130.0 MPa | O | EN 573-3 | Flat |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil | |
100 °C | 2.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.35e-05 1/K | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil | ||
100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | 20-100°C | |
Conductividad térmica | 201 W/(m·K) Show Material materials with Conductividad térmica of 201 W/(m·K) | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | ||
20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 210.0 - 220.0 W/(m·K) | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate | ||
Temperatura de fusión | 640.0 - 655.0 °C Show Material materials with Temperatura de fusión of 640.0 - 655.0 °C | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 34000000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 34000000.0 - 35000000.0 S/m | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
Resistividad eléctrica | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.86e-08 - 2.94e-08 Ω·m | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Strip, Sheet, Plate, Foil | |
3e-08 - 3.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3e-08 - 3.5e-08 Ω·m | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.1 % Show Material materials with Cobre of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.1 % Show Material materials with Cromo of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | |
Hierro | 0.5 - 1.0 % Show Material materials with Hierro of 0.5 - 1.0 % | O | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Coil, Sheet, Strip, Foil, Plate |
Magnesio | 0.1 % Show Material materials with Magnesio of 0.1 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.1 % Show Material materials with Magnesio of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.1 % Show Material materials with Manganeso of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % | O | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Coil, Sheet, Strip, Foil, Plate |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.05 % Show Material materials with Titanio of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil | |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | O | EN 573-3, EN 1396, EN 485, EN 546, EN 683 | Sheet, Strip, Foil, Flat, Plate |
0.1 % Show Material materials with Zinc of 0.1 % | O | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 683-2, EN 541, EN 546-2 | Coil, Sheet, Strip, Foil |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Interiors and ceilings: Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins, General applications; Tubes: Flexible tube, Pipes; Insulation; Closures: Long cups, Short cups, Easy open; Cosmetic: Cosmetic pieces; Pharmacy: Pharma and para-pharma; Semi-rigid and corrugated: Pet food, Smooth wall; Foil stock: Foil app | |
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good | |
Corrosion properties | Moderated | |
Welding | Excellent | |
Workability | Excellent |