General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.73 g/cm³ Show Material materials with Densidad of 2.73 g/cm³ | O | EN 573-3, EN 546 | Foil |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 8000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 70.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 130.0 MPa | O | EN 573-3, EN 546 | Foil | |
20.0 °C | 70.0 - 135.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 135.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 140.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 140.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 145.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 145.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 135.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 135.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 75.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 130.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 140.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 140.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 145.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 145.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 80.0 - 135.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 135.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 80.0 - 130.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 130.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 80.0 - 140.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 140.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 80.0 - 145.0 MPa Show Material materials with Resistencia a la tracción of 80.0 - 145.0 MPa | O | EN 573-3 | Foil |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium |
Coeficiente de dilatación térmica | 1.9e-05 - 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.1e-05 1/K | Typical for Wrought 8000 Series Aluminium |
Conductividad térmica | 167.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 167.0 - 220.0 W/(m·K) | Typical for Wrought 8000 Series Aluminium |
Temperatura de fusión | 645.0 - 655.0 °C Show Material materials with Temperatura de fusión of 645.0 - 655.0 °C | Typical for Wrought 8000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 28000000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 28000000.0 - 35000000.0 S/m | Typical for Wrought 8000 Series Aluminium |
Resistividad eléctrica | 2.8e-08 - 3.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.8e-08 - 3.5e-08 Ω·m | Typical for Wrought 8000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | O | EN 573-3, EN 546 | Foil |
Hierro | 1.2 - 1.6 % Show Material materials with Hierro of 1.2 - 1.6 % | O | EN 573-3, EN 546 | Foil |
Magnesio | 0.1 % Show Material materials with Magnesio of 0.1 % | O | EN 573-3, EN 546 | Foil |
Manganeso | 0.2 - 0.6 % Show Material materials with Manganeso of 0.2 - 0.6 % | O | EN 573-3, EN 546 | Foil |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % | O | EN 573-3, EN 546 | Foil |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | O | EN 573-3, EN 546 | Foil |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | O | EN 573-3, EN 546 | Foil |