General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil |
2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | O | EN 573-3, EN 546 | Foil |
Medidas
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 8000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 60.0 - 100.0 MPa Show Material materials with Resistencia a la tracción of 60.0 - 100.0 MPa | O | EN 573-3, EN 546 | Foil | |
20.0 °C | 60.0 - 105.0 MPa Show Material materials with Resistencia a la tracción of 60.0 - 105.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 60.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 60.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 105.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 105.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 65.0 - 100.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 65.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 65.0 - 110.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 110.0 MPa | O | EN 573-3, EN 546 | Foil | ||
20.0 °C | 70.0 - 100.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 70.0 - 105.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 105.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 110.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 110.0 MPa | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2, EN 573-3, EN 546 | Coil, Foil, Foil | ||
20.0 °C | 75.0 - 100.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 100.0 MPa | O | EN 573-3 | Foil | ||
20.0 °C | 75.0 - 105.0 MPa Show Material materials with Resistencia a la tracción of 75.0 - 105.0 MPa | O | EN 573-3 | Foil |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Conductividad térmica | 167.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 167.0 - 220.0 W/(m·K) | Typical for Wrought 8000 Series Aluminium | ||||
Temperatura de fusión | 645.0 - 655.0 °C Show Material materials with Temperatura de fusión of 645.0 - 655.0 °C | Typical for Wrought 8000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 28000000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 28000000.0 - 35000000.0 S/m | Typical for Wrought 8000 Series Aluminium |
Resistividad eléctrica | 2.8e-08 - 3.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.8e-08 - 3.5e-08 Ω·m | Typical for Wrought 8000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Cobre of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Cromo | 0.03 % Show Material materials with Cromo of 0.03 % | O | EN 573-3, EN 546 | Foil |
0.03 % Show Material materials with Cromo of 0.03 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Hierro | 1.1 - 1.7 % Show Material materials with Hierro of 1.1 - 1.7 % | O | EN 573-3, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Foil, Coil, Foil |
Magnesio | 0.01 % Show Material materials with Magnesio of 0.01 % | O | EN 573-3, EN 546 | Foil |
0.01 % Show Material materials with Magnesio of 0.01 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Manganeso | 0.03 % Show Material materials with Manganeso of 0.03 % | O | EN 573-3, EN 546 | Foil |
0.03 % Show Material materials with Manganeso of 0.03 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | O | EN 573-3, EN 546 | Foil |
0.4 % Show Material materials with Silicona of 0.4 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Titanio of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil | |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | O | EN 573-3, EN 546 | Foil |
0.05 % Show Material materials with Zinc of 0.05 % | O | EN 573-1, EN 573-2, EN 573-3, EN 546-2 | Coil, Foil |
Technological properties
Property | ||
---|---|---|
Application areas | Foil stock: Foil app | |
Workability | Excellent |