General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil |
2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | H19 | EN 573-3, EN 683 | Foil |
Medidas
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Límite elástico | 155.0 MPa Show Material materials with Límite elástico of 155.0 MPa | H19 | EN 573-3, EN 683 | Foil | RP02 | |
155 MPa Show Material materials with Límite elástico of 155 MPa | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil | |||
20.0 °C | 155.0 MPa Show Material materials with Límite elástico of 155.0 MPa | H19 | EN 573-3 | Foil | RP02 | |
Módulo elástico | 69.0 - 72.0 GPa Show Material materials with Módulo elástico of 69.0 - 72.0 GPa | Typical for Wrought 8000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Resistencia a la tracción | 170.0 - 175.0 MPa Show Material materials with Resistencia a la tracción of 170.0 - 175.0 MPa | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil | ||
170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | H19 | EN 573-3, EN 683 | Foil | |||
20.0 °C | 170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | H19 | EN 573-3 | Foil | ||
20.0 °C | 175.0 MPa Show Material materials with Resistencia a la tracción of 175.0 MPa | H19 | EN 573-3 | Foil |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil | |
Conductividad térmica | 167.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 167.0 - 220.0 W/(m·K) | Typical for Wrought 8000 Series Aluminium | ||||
Temperatura de fusión | 645.0 - 655.0 °C Show Material materials with Temperatura de fusión of 645.0 - 655.0 °C | Typical for Wrought 8000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 28000000.0 - 35000000.0 S/m Show Material materials with Conductividad eléctrica of 28000000.0 - 35000000.0 S/m | Typical for Wrought 8000 Series Aluminium |
Resistividad eléctrica | 2.8e-08 - 3.5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.8e-08 - 3.5e-08 Ω·m | Typical for Wrought 8000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | H19 | EN 573-3, EN 683 | Foil |
0.05 % Show Material materials with Cobre of 0.05 % | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil | |
Hierro | 0.7 - 1.3 % Show Material materials with Hierro of 0.7 - 1.3 % | H19 | EN 573-3, EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3, EN 683 | Foil |
Silicona | 0.05 - 0.3 % Show Material materials with Silicona of 0.05 - 0.3 % | H19 | EN 573-3, EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3, EN 683 | Foil |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H19 | EN 573-3, EN 683 | Foil |
0.1 % Show Material materials with Zinc of 0.1 % | H19 | EN 546-2, EN 683-2, EN 573-1, EN 573-2, EN 573-3 | Foil |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing: Foil for bituminous coating; Heat exchangers: Fins, Heat exchangers; Insulation; Semi-rigid and corrugated: Pet food; Foil stock: Foil app; Components: Automotive fins, Heat exchangers | |
Corrosion properties | Moderated | |
Workability | Excellent |