General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
20.0 °C | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | H24 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Coil, Sheet |
Medidas
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Espesor | 0.04 mm Show Material materials with Espesor of 0.04 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | 0.04 mm | Coil, Sheet |
1.5 mm Show Material materials with Espesor of 1.5 mm | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | 1.5 mm | Coil, Sheet |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Dureza Brinell | 52.0 [-] Show Material materials with Dureza Brinell of 52.0 [-] | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 52.0 [-] Show Material materials with Dureza Brinell of 52.0 [-] | H24 | EN 573-3 | Flat | ||
Dureza Brinell (HBW) | 53 [-] Show Material materials with Dureza Brinell (HBW) of 53 [-] | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
Elongación | 1.0 - 3.0 % Show Material materials with Elongación of 1.0 - 3.0 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | A50 | |
3.0 % Show Material materials with Elongación of 3.0 % | H24 | EN 573-3, EN 546 | Strip, Sheet, Plate, Welded Tube | A50 | ||
4.0 % Show Material materials with Elongación of 4.0 % | H24 | EN 573-3, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | A50 | ||
7.0 % Show Material materials with Elongación of 7.0 % | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | A100 | ||
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H24 | EN 573-3 | Foil | A100 | |
20.0 °C | 3.0 % Show Material materials with Elongación of 3.0 % | H24 | EN 573-3 | Foil | A50 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H24 | EN 573-3 | Foil | A100 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H24 | EN 573-3 | Flat, Foil | A50 | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | H24 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | H24 | EN 573-3 | Seamless Tube | ||
Límite elástico | 45 MPa Show Material materials with Límite elástico of 45 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
130.0 MPa Show Material materials with Límite elástico of 130.0 MPa | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | RP02 | ||
175.0 MPa Show Material materials with Límite elástico of 175.0 MPa | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | RP02 | ||
20.0 °C | 130.0 MPa Show Material materials with Límite elástico of 130.0 MPa | H24 | EN 573-3 | Flat | RP02 Transverse | |
20.0 °C | 130.0 MPa Show Material materials with Límite elástico of 130.0 MPa | H24 | EN 573-3 | Flat | RP02 | |
20.0 °C | 175.0 MPa Show Material materials with Límite elástico of 175.0 MPa | H24 | EN 573-3 | Seamless Tube | RP02 | |
Módulo de cizallamiento | 26.0 GPa Show Material materials with Módulo de cizallamiento of 26.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
20.0 °C | 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.5 GPa | H24 | EN 573-3 | Foil, Flat, Seamless Tube | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Resistencia a la tracción | 125.0 - 225.0 MPa Show Material materials with Resistencia a la tracción of 125.0 - 225.0 MPa | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | ||
200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | H24 | EN 573-3, EN 1592 | Strip, Sheet, Plate, Welded Tube | |||
20.0 °C | 170.0 - 215.0 MPa Show Material materials with Resistencia a la tracción of 170.0 - 215.0 MPa | H24 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 170.0 - 215.0 MPa Show Material materials with Resistencia a la tracción of 170.0 - 215.0 MPa | H24 | EN 573-3 | Flat | Transverse | |
20.0 °C | 180.0 - 225.0 MPa Show Material materials with Resistencia a la tracción of 180.0 - 225.0 MPa | H24 | EN 573-3, EN 546 | Foil, Strip, Sheet, Plate, Welded Tube | ||
20.0 °C | 200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | H24 | EN 573-3 | Seamless Tube | ||
Ángulo de flexión a 180° | 1.5 °/t Show Material materials with Ángulo de flexión a 180° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
1.5 °/t Show Material materials with Ángulo de flexión a 180° of 1.5 °/t | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
Ángulo de flexión a 90° | 0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | ||
0.5 °/t Show Material materials with Ángulo de flexión a 90° of 0.5 °/t | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
1.0 °/t Show Material materials with Ángulo de flexión a 90° of 1.0 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube | |||
1.5 °/t Show Material materials with Ángulo de flexión a 90° of 1.5 °/t | H24 | EN 573-3, EN 485 | Strip, Sheet, Plate, Welded Tube |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 893.0 J/(kg·K) Show Material materials with Calor específico of 893.0 J/(kg·K) | H24 | EN 573-3 | Foil, Flat, Seamless Tube | |
Coeficiente de dilatación térmica | 20 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | ||
100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | 20-100°C | |
Conductividad térmica | 160.0 - 190.0 W/(m·K) Show Material materials with Conductividad térmica of 160.0 - 190.0 W/(m·K) | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | ||
172 W/(m·K) Show Material materials with Conductividad térmica of 172 W/(m·K) | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |||
20.0 °C | 200.0 W/(m·K) Show Material materials with Conductividad térmica of 200.0 W/(m·K) | H24 | EN 573-3 | Foil, Flat, Seamless Tube | ||
Temperatura de fusión | 630.0 - 654.0 °C Show Material materials with Temperatura de fusión of 630.0 - 654.0 °C | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 23000000.0 - 25000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 25000000.0 S/m | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
20.0 °C | 28000000.0 S/m Show Material materials with Conductividad eléctrica of 28000000.0 S/m | H24 | EN 573-3 | Foil, Flat, Seamless Tube | |
Resistividad eléctrica | 3.7999999999999996e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.7999999999999996e-08 Ω·m | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
4e-08 - 4.35e-08 Ω·m Show Material materials with Resistividad eléctrica of 4e-08 - 4.35e-08 Ω·m | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.3 % Show Material materials with Cobre of 0.3 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.1 % Show Material materials with Cromo of 0.1 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | H24 | EN 573-3 | Foil, Flat, Seamless Tube |
0.70 % Show Material materials with Hierro of 0.70 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Strip, Sheet, Plate, Welded Tube | |
0.7 % Show Material materials with Hierro of 0.7 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Magnesio | 0.2 - 0.6 % Show Material materials with Magnesio of 0.2 - 0.6 % | H24 | EN 573-3, EN 1592, EN 485, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube, Coil, Sheet |
Manganeso | 1.0 - 1.5 % Show Material materials with Manganeso of 1.0 - 1.5 % | H24 | EN 573-3, EN 1592, EN 485, EN 546, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube, Coil, Sheet |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.6 % Show Material materials with Silicona of 0.6 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet | |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H24 | EN 573-3, EN 1592, EN 485, EN 546 | Foil, Flat, Seamless Tube, Strip, Sheet, Plate, Welded Tube |
0.25 % Show Material materials with Zinc of 0.25 % | H24 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 546-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Electronic devices: Housing of devices; Insulation; Cosmetics: Cosmetics pieces | |
Brazing | Good | |
Corrosion properties | Seawater: very good, weathering: very good | |
Welding | Good | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) very good (O) / acceptable (H12) |