General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Módulo de cizallamiento | 25.0 - 26.0 GPa Show Material materials with Módulo de cizallamiento of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium | ||||
Módulo elástico | 69.5 - 70.0 GPa Show Material materials with Módulo elástico of 69.5 - 70.0 GPa | Typical for Wrought 3000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 260.0 - 330.0 MPa Show Material materials with Resistencia a la tracción of 260.0 - 330.0 MPa | H19 | EN 573-3 | Sheet | |
20.0 °C | 260.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 260.0 - 300.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 260.0 - 310.0 MPa Show Material materials with Resistencia a la tracción of 260.0 - 310.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 270.0 - 330.0 MPa Show Material materials with Resistencia a la tracción of 270.0 - 330.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 270.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 270.0 - 300.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 270.0 - 310.0 MPa Show Material materials with Resistencia a la tracción of 270.0 - 310.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 290.0 - 330.0 MPa Show Material materials with Resistencia a la tracción of 290.0 - 330.0 MPa | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | ||
20.0 °C | 290.0 - 300.0 MPa Show Material materials with Resistencia a la tracción of 290.0 - 300.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 290.0 - 310.0 MPa Show Material materials with Resistencia a la tracción of 290.0 - 310.0 MPa | H19 | EN 573-3 | Sheet |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 893.0 - 920.0 J/(kg·K) Show Material materials with Calor específico of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium |
Coeficiente de dilatación térmica | 2.2e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium |
Conductividad térmica | 154.0 - 193.0 W/(m·K) Show Material materials with Conductividad térmica of 154.0 - 193.0 W/(m·K) | Typical for Wrought 3000 Series Aluminium |
Temperatura de fusión | 629.0 - 654.0 °C Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 23000000.0 - 29000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.05 - 0.25 % Show Material materials with Cobre of 0.05 - 0.25 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Galio | 0.05 % Show Material materials with Galio of 0.05 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | H19 | EN 573-3 | Sheet |
0.80 % Show Material materials with Hierro of 0.80 % | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Magnesio | 0.8 - 1.3 % Show Material materials with Magnesio of 0.8 - 1.3 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Manganeso | 0.8 - 1.4 % Show Material materials with Manganeso of 0.8 - 1.4 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |