General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | H28 | EN 573-3, EN 541 | Strip, Sheet, Plate |
Medidas
Property | Value | Condition | Related Standards | Thickness | Shape |
---|---|---|---|---|---|
Espesor | 0.18 mm Show Material materials with Espesor of 0.18 mm | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | 0.18 mm | Coil, Sheet |
0.30 mm Show Material materials with Espesor of 0.30 mm | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | 0.30 mm | Coil, Sheet |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Límite elástico | 120.0 - 220.0 MPa Show Material materials with Límite elástico of 120.0 - 220.0 MPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 170.0 - 220.0 MPa Show Material materials with Límite elástico of 170.0 - 220.0 MPa | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate | RP02 | |
Módulo de cizallamiento | 26.0 GPa Show Material materials with Módulo de cizallamiento of 26.0 GPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Resistencia a la tracción | 150.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 150.0 - 240.0 MPa | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
20.0 °C | 190.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 190.0 - 240.0 MPa | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 893.0 - 920.0 J/(kg·K) Show Material materials with Calor específico of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium | ||||
Coeficiente de dilatación térmica | 100 °C | 0.000024 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000024 1/K | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | 20-100°C |
Conductividad térmica | 172 W/(m·K) Show Material materials with Conductividad térmica of 172 W/(m·K) | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | ||
Temperatura de fusión | 629.0 - 654.0 °C Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Conductividad eléctrica | 23000000.0 - 29000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium | |||
Resistividad eléctrica | 3.7999999999999996e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.7999999999999996e-08 Ω·m | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.3 % Show Material materials with Cobre of 0.3 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Cromo | 0.2 % Show Material materials with Cromo of 0.2 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.2 % Show Material materials with Cromo of 0.2 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | H28 | EN 573-3 | Sheet |
0.7 % Show Material materials with Hierro of 0.7 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
0.70 % Show Material materials with Hierro of 0.70 % | H28 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Magnesio | 0.2 - 0.8 % Show Material materials with Magnesio of 0.2 - 0.8 % | H28 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Manganeso | 0.3 - 0.8 % Show Material materials with Manganeso of 0.3 - 0.8 % | H28 | EN 573-3, EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541, EN 541 | Sheet, Coil, Sheet, Strip, Plate |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.6 % Show Material materials with Silicona of 0.6 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet | |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H28 | EN 573-3, EN 541 | Sheet, Strip, Plate |
0.25 % Show Material materials with Zinc of 0.25 % | H28 | EN 573-1, EN 573-2, EN 573-3, EN 485-2, EN 541 | Coil, Sheet |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Closures: Short cups; Food can: Body, Lids; Semi-rigid and corrugated: Pet food | |
Brazing | Good | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |