General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.73 g/cm³ Show Material materials with Densidad of 2.73 g/cm³ | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
20.0 °C | 2.71 g/cm³ Show Material materials with Densidad of 2.71 g/cm³ | H19 | EN 573-3 | Sheet |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 3000 Series Aluminium | ||||
Módulo de cizallamiento | 20.0 °C | 26.5 Show Material materials with Módulo de cizallamiento of 26.5 | H19 | EN 573-3 | Sheet | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 180.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 180.0 - 240.0 MPa | H19 | EN 573-3 | Sheet | |
20.0 °C | 180.0 - 230.0 MPa Show Material materials with Resistencia a la tracción of 180.0 - 230.0 MPa | H19 | EN 573-3 | Sheet | ||
20.0 °C | 200.0 - 240.0 MPa Show Material materials with Resistencia a la tracción of 200.0 - 240.0 MPa | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | ||
20.0 °C | 200.0 - 230.0 MPa Show Material materials with Resistencia a la tracción of 200.0 - 230.0 MPa | H19 | EN 573-3 | Sheet |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 20.0 °C | 893.0 J/(kg·K) Show Material materials with Calor específico of 893.0 J/(kg·K) | H19 | EN 573-3 | Sheet | |
Coeficiente de dilatación térmica | 2.2e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium | ||||
Conductividad térmica | 20.0 °C | 200.0 Show Material materials with Conductividad térmica of 200.0 | H19 | EN 573-3 | Sheet | |
Temperatura de fusión | 629.0 - 654.0 °C Show Material materials with Temperatura de fusión of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 28000000.0 Show Material materials with Conductividad eléctrica of 28000000.0 | H19 | EN 573-3 | Sheet | |
Resistividad eléctrica | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Hierro | 0.45 % Show Material materials with Hierro of 0.45 % | H19 | EN 573-3 | Sheet |
0.45 % Show Material materials with Hierro of 0.45 % | H19 | EN 573-3, EN 541 | Strip, Sheet, Plate | |
Magnesio | 0.1 % Show Material materials with Magnesio of 0.1 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Manganeso | 0.4 - 0.8 % Show Material materials with Manganeso of 0.4 - 0.8 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H19 | EN 573-3, EN 541 | Sheet, Strip, Plate |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: sufficient, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good | |
Corrosion properties | Seawater: good, weathering: very good | |
Workability | Bending / Spinning (cold): very good / very good, Impact extrusion (cold): good, Deep drawing / upsetting (Condition) very good (O) / very good (H12) |