General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T6 | ISO 3522 | |
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||
Dureza Brinell | 115.0 [-] Show Material materials with Dureza Brinell of 115.0 [-] | T6 | ISO 3522 | |
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | ||
Resistencia a la tracción | 480.0 MPa Show Material materials with Resistencia a la tracción of 480.0 MPa | T6 | ISO 3522 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium | |||
Coeficiente de dilatación térmica | 20 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T6 | ISO 3522 | |
100 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T6 | ISO 3522 | ||
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | T6 | ISO 3522 | ||
Temperatura de fusión | 510.0 - 790.0 °C Show Material materials with Temperatura de fusión of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | T6 | ISO 3522 |
Resistividad eléctrica | 4.35e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.35e-08 - 6.25e-08 Ω·m | T6 | ISO 3522 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 4.0 - 5.0 % Show Material materials with Cobre of 4.0 - 5.0 % | T6 | ISO 3522 |
Hierro | 0.10 % Show Material materials with Hierro of 0.10 % | T6 | ISO 3522 |
Magnesio | 0.15 - 0.35 % Show Material materials with Magnesio of 0.15 - 0.35 % | T6 | ISO 3522 |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % | T6 | ISO 3522 |
Plata | 0.4 - 1.0 % Show Material materials with Plata of 0.4 - 1.0 % | T6 | ISO 3522 |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % | T6 | ISO 3522 |
Titanio | 0.15 - 0.35 % Show Material materials with Titanio of 0.15 - 0.35 % | T6 | ISO 3522 |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | T6 | ISO 3522 |