Chemical properties
Property | Value |
---|---|
Bismuto | 0.4 % Show Material materials with Bismuto of 0.4 % |
Cobre | 4.5 % Show Material materials with Cobre of 4.5 % |
Cromo | 0.15 % Show Material materials with Cromo of 0.15 % |
Estaño | 1.3 % Show Material materials with Estaño of 1.3 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Magnesio | 1.1 % Show Material materials with Magnesio of 1.1 % |
Manganeso | 0.8 % Show Material materials with Manganeso of 0.8 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |