General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.65 g/cm³ Show Material materials with Densidad of 2.65 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 20.0 °C | 65 - 75 GPa Show Material materials with Módulo elástico of 65 - 75 GPa |
Chemical properties
Property | Value |
---|---|
Circonio | 0.3 % Show Material materials with Circonio of 0.3 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Magnesio | 0.08 % Show Material materials with Magnesio of 0.08 % |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % |
Silicona | 10.5 % Show Material materials with Silicona of 10.5 % |
Titanio | 0.06 % Show Material materials with Titanio of 0.06 % |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % |
Zinc | 0.07 % Show Material materials with Zinc of 0.07 % |