General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.74 g/cm³ Show Material materials with Densidad of 2.74 g/cm³ | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 4000 Series Aluminium | ||||
Dureza Brinell | 32.0 [-] Show Material materials with Dureza Brinell of 32.0 [-] | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate | ||
20.0 °C | 32.0 [-] Show Material materials with Dureza Brinell of 32.0 [-] | H111 | EN 573-3 | Flat | ||
Módulo de cizallamiento | 26.0 GPa Show Material materials with Módulo de cizallamiento of 26.0 GPa | Typical for Wrought 4000 Series Aluminium | ||||
Módulo elástico | 69.0 - 71.0 GPa Show Material materials with Módulo elástico of 69.0 - 71.0 GPa | Typical for Wrought 4000 Series Aluminium | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium | ||||
Resistencia a la tracción | 20.0 °C | 110.0 - 150.0 MPa Show Material materials with Resistencia a la tracción of 110.0 - 150.0 MPa | H111 | EN 573-3 | Flat | Transverse |
20.0 °C | 110.0 - 150.0 MPa Show Material materials with Resistencia a la tracción of 110.0 - 150.0 MPa | H111 | EN 573-3, EN 485 | Strip, Sheet, Plate, Flat |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 864.0 J/(kg·K) Show Material materials with Calor específico of 864.0 J/(kg·K) | Typical for Wrought 4000 Series Aluminium |
Coeficiente de dilatación térmica | 1.2e-05 - 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2e-05 - 2.2e-05 1/K | Typical for Wrought 4000 Series Aluminium |
Conductividad térmica | 138.0 - 155.0 W/(m·K) Show Material materials with Conductividad térmica of 138.0 - 155.0 W/(m·K) | Typical for Wrought 4000 Series Aluminium |
Temperatura de fusión | 520.0 - 630.0 °C Show Material materials with Temperatura de fusión of 520.0 - 630.0 °C | Typical for Wrought 4000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 23000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 23000000.0 - 30000000.0 S/m | Typical for Wrought 4000 Series Aluminium |
Resistividad eléctrica | 3.8e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.8e-08 - 5e-08 Ω·m | Typical for Wrought 4000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobalto | 0.05 % Show Material materials with Cobalto of 0.05 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Cromo | 0.05 - 0.25 % Show Material materials with Cromo of 0.05 - 0.25 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Hierro | 0.4 - 1.0 % Show Material materials with Hierro of 0.4 - 1.0 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Magnesio | 0.2 % Show Material materials with Magnesio of 0.2 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Manganeso | 0.8 - 1.5 % Show Material materials with Manganeso of 0.8 - 1.5 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Níquel | 0.15 - 0.7 % Show Material materials with Níquel of 0.15 - 0.7 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Silicona | 1.0 - 1.7 % Show Material materials with Silicona of 1.0 - 1.7 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H111 | EN 573-3, EN 485 | Flat, Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |