General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Densidad | 20.0 °C | 2.66 g/cm³ Show Material materials with Densidad of 2.66 g/cm³ | T64 | EN 1706 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T64 | EN 1706, EN 13195 | Casting | ||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||||
Dureza Brinell | 90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T64 | EN 1706, EN 13195 | Casting | ||
20.0 °C | 90.0 [-] Show Material materials with Dureza Brinell of 90.0 [-] | T64 | EN 1706 | |||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||||
Módulo elástico | 20.0 °C | 69.0 - 75.0 GPa Show Material materials with Módulo elástico of 69.0 - 75.0 GPa | T64 | EN 1706 | ||
Resistencia a la tracción | 290.0 MPa Show Material materials with Resistencia a la tracción of 290.0 MPa | T64 | EN 1706, EN 13195 | Casting | ||
20.0 °C | 290.0 MPa Show Material materials with Resistencia a la tracción of 290.0 MPa | T64 | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T64 | EN 1706, EN 13195 | Casting | |
100.0 °C | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T64 | EN 1706, EN 13195 | Casting | ||
100 °C | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T64 | EN 1706, EN 13195 | Casting | ||
Conductividad térmica | 20.0 °C | 150.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 - 180.0 W/(m·K) | T64 | EN 1706, EN 13195 | Casting | |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 20000000.0 - 26000000.0 S/m Show Material materials with Conductividad eléctrica of 20000000.0 - 26000000.0 S/m | T64 | EN 1706, EN 13195 | Casting |
Resistividad eléctrica | 3.85e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.85e-08 - 5e-08 Ω·m | T64 | EN 1706, EN 13195 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 91.04 % Show Material materials with Aluminio of 91.04 % | T64 | EN 1706 | |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | T64 | EN 1706, EN 13195 | Casting |
Hierro | 0.19 % Show Material materials with Hierro of 0.19 % | T64 | EN 1706 | |
0.19 % Show Material materials with Hierro of 0.19 % | T64 | EN 1706, EN 13195 | Casting | |
Magnesio | 0.45 - 0.7 % Show Material materials with Magnesio of 0.45 - 0.7 % | T64 | EN 1706, EN 13195 | Casting |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T64 | EN 1706, EN 13195 | Casting |
Silicona | 6.5 - 7.5 % Show Material materials with Silicona of 6.5 - 7.5 % | T64 | EN 1706, EN 13195 | Casting |
Titanio | 0.08 - 0.25 % Show Material materials with Titanio of 0.08 - 0.25 % | T64 | EN 1706, EN 13195 | Casting |
Zinc | 0.07 % Show Material materials with Zinc of 0.07 % | T64 | EN 1706, EN 13195 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not sufficient | |
Corrosion properties | general: good | |
General machinability | as cast: good | |
Processing methods | permanent mould casting, separately cast test sample |