General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 60.0 - 90.0 MPa Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa | F | EN 1706 | Casting | ||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||||
Dureza Brinell | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | F | EN 1706 | Casting | ||
20.0 °C | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | F | EN 1706 | |||
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||||
Resistencia a la tracción | 180.0 MPa Show Material materials with Resistencia a la tracción of 180.0 MPa | F | EN 1706 | Casting | ||
20.0 °C | 180.0 MPa Show Material materials with Resistencia a la tracción of 180.0 MPa | F | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | F | EN 1706 | Casting | |
100.0 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | F | EN 1706 | Casting | ||
100 °C | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | F | EN 1706 | Casting | ||
Conductividad térmica | 20.0 °C | 110.0 - 120.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 - 120.0 W/(m·K) | F | EN 1706 | Casting | |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 14000000.0 - 17000000.0 S/m Show Material materials with Conductividad eléctrica of 14000000.0 - 17000000.0 S/m | F | EN 1706 | Casting |
Resistividad eléctrica | 5.88e-08 - 7.14e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.88e-08 - 7.14e-08 Ω·m | F | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 84.25 % Show Material materials with Aluminio of 84.25 % | F | EN 1706 | |
Cobre | 3.0 - 4.0 % Show Material materials with Cobre of 3.0 - 4.0 % | F | EN 1706 | Casting |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % | F | EN 1706 | Casting |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % | F | EN 1706 | |
0.80 % Show Material materials with Hierro of 0.80 % | F | EN 1706 | Casting | |
Magnesio | 0.3 - 0.6 % Show Material materials with Magnesio of 0.3 - 0.6 % | F | EN 1706 | Casting |
Manganeso | 0.2 - 0.65 % Show Material materials with Manganeso of 0.2 - 0.65 % | F | EN 1706 | Casting |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % | F | EN 1706 | Casting |
Plomo | 0.15 % Show Material materials with Plomo of 0.15 % | F | EN 1706 | Casting |
Silicona | 6.5 - 8.0 % Show Material materials with Silicona of 6.5 - 8.0 % | F | EN 1706 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | F | EN 1706 | Casting |
Zinc | 0.65 % Show Material materials with Zinc of 0.65 % | F | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: acceptable | |
General machinability | after thermal treatment: acceptable | |
Processing methods | permanent mould casting, separately cast test sample |