Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 546 - 621 °C Show Material materials with Temperatura de fusión of 546 - 621 °C |
Chemical properties
Property | Value |
---|---|
Cobre | 1.5 % Show Material materials with Cobre of 1.5 % |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % |
Hierro | 0.6 % Show Material materials with Hierro of 0.6 % |
Magnesio | 0.6 % Show Material materials with Magnesio of 0.6 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Silicona | 5.5 % Show Material materials with Silicona of 5.5 % |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % |