General
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Densidad | 20.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | F | EN 1706 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 60.0 - 90.0 MPa Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa | F | EN 1706 | Casting | ||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | ||||
Dureza Brinell | 50.0 [-] Show Material materials with Dureza Brinell of 50.0 [-] | F | EN 1706 | Casting | ||
20.0 °C | 50.0 [-] Show Material materials with Dureza Brinell of 50.0 [-] | F | EN 1706 | |||
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | ||||
Resistencia a la tracción | 140.0 MPa Show Material materials with Resistencia a la tracción of 140.0 MPa | F | EN 1706 | Casting | ||
150.0 MPa Show Material materials with Resistencia a la tracción of 150.0 MPa | F | EN 1706 | Casting | |||
20.0 °C | 140.0 MPa Show Material materials with Resistencia a la tracción of 140.0 MPa | F | EN 1706 | |||
20.0 °C | 150.0 MPa Show Material materials with Resistencia a la tracción of 150.0 MPa | F | EN 1706 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium | ||||
Coeficiente de dilatación térmica | 20 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | F | EN 1706 | Casting | |
100.0 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | F | EN 1706 | Casting | ||
100 °C | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | F | EN 1706 | Casting | ||
Conductividad térmica | 20.0 °C | 130.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 140.0 W/(m·K) | F | EN 1706 | Casting | |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 17000000.0 - 22000000.0 S/m Show Material materials with Conductividad eléctrica of 17000000.0 - 22000000.0 S/m | F | EN 1706 | Casting |
Resistividad eléctrica | 4.55e-08 - 5.88e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.55e-08 - 5.88e-08 Ω·m | F | EN 1706 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 94.4 % Show Material materials with Aluminio of 94.4 % | F | EN 1706 | |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | F | EN 1706 | Casting |
Hierro | 0.55 % Show Material materials with Hierro of 0.55 % | F | EN 1706 | |
0.55 % Show Material materials with Hierro of 0.55 % | F | EN 1706 | Casting | |
Magnesio | 2.5 - 3.5 % Show Material materials with Magnesio of 2.5 - 3.5 % | F | EN 1706 | Casting |
Manganeso | 0.45 % Show Material materials with Manganeso of 0.45 % | F | EN 1706 | Casting |
Silicona | 0.55 % Show Material materials with Silicona of 0.55 % | F | EN 1706 | Casting |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | F | EN 1706 | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | F | EN 1706 | Casting |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: excellent | |
Corrosion properties | general: excellent | |
General machinability | after thermal treatment: excellent | |
Processing methods | permanent mould casting, separately cast test sample |