General
Property | Value | Comment |
---|---|---|
Densidad | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Dureza Brinell | 80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | F | GB 1173 | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Módulo elástico | 73.0 - 80.0 GPa Show Material materials with Módulo elástico of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Resistencia a la tracción | 205.0 MPa Show Material materials with Resistencia a la tracción of 205.0 MPa | F | GB 1173 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 960.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Coeficiente de dilatación térmica | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Conductividad térmica | 130.0 - 180.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Temperatura de fusión | 505.0 - 770.0 °C Show Material materials with Temperatura de fusión of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Cobre | 1.3 - 1.8 % Show Material materials with Cobre of 1.3 - 1.8 % | F | GB 1173 |
Estaño | 0.01 % Show Material materials with Estaño of 0.01 % | F | GB 1173 |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | F | GB 1173 |
Magnesio | 0.4 - 0.6 % Show Material materials with Magnesio of 0.4 - 0.6 % | F | GB 1173 |
Manganeso | 0.1 - 0.35 % Show Material materials with Manganeso of 0.1 - 0.35 % | F | GB 1173 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % | F | GB 1173 |
Silicona | 8.0 - 10.0 % Show Material materials with Silicona of 8.0 - 10.0 % | F | GB 1173 |
Titanio | 0.1 - 0.35 % Show Material materials with Titanio of 0.1 - 0.35 % | F | GB 1173 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | F | GB 1173 |