General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 - 2.8 g/cm³ Show Material materials with Densidad of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||
Dureza Brinell | 70.0 [-] Show Material materials with Dureza Brinell of 70.0 [-] | T51 | GB 1173 | |
Módulo elástico | 72.0 GPa Show Material materials with Módulo elástico of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | ||
Resistencia a la tracción | 215.0 MPa Show Material materials with Resistencia a la tracción of 215.0 MPa | T51 | GB 1173 | |
225.0 MPa Show Material materials with Resistencia a la tracción of 225.0 MPa | T51 | GB 1173 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 875.0 - 963.0 J/(kg·K) Show Material materials with Calor específico of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Coeficiente de dilatación térmica | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Conductividad térmica | 120.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Temperatura de fusión | 510.0 - 790.0 °C Show Material materials with Temperatura de fusión of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Circonio | 0.1 % Show Material materials with Circonio of 0.1 % | T51 | GB 1173 |
Cobre | 4.0 - 5.0 % Show Material materials with Cobre of 4.0 - 5.0 % | T51 | GB 1173 |
Estaño | 0.01 % Show Material materials with Estaño of 0.01 % | T51 | GB 1173 |
Hierro | 0.80 % Show Material materials with Hierro of 0.80 % | T51 | GB 1173 |
Magnesio | 0.05 % Show Material materials with Magnesio of 0.05 % | T51 | GB 1173 |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T51 | GB 1173 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % | T51 | GB 1173 |
Silicona | 1.2 % Show Material materials with Silicona of 1.2 % | T51 | GB 1173 |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | T51 | GB 1173 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T51 | GB 1173 |