General
Property | Value | Comment |
---|---|---|
Densidad | 2.75 g/cm³ Show Material materials with Densidad of 2.75 g/cm³ | Typical for Cast 1xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 1xx.x Series Aluminium | ||
Dureza Brinell | 75.0 [-] Show Material materials with Dureza Brinell of 75.0 [-] | T5 | GB 1173 | |
Módulo elástico | 70.0 GPa Show Material materials with Módulo elástico of 70.0 GPa | Typical for Cast 1xx.x Series Aluminium | ||
Resistencia a la tracción | 165.0 MPa Show Material materials with Resistencia a la tracción of 165.0 MPa | T5 | GB 1173 | |
175.0 MPa Show Material materials with Resistencia a la tracción of 175.0 MPa | T5 | GB 1173 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 1.8e-05 - 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8e-05 - 2.4e-05 1/K | Typical for Cast 1xx.x Series Aluminium |
Conductividad térmica | 209.0 - 222.0 W/(m·K) Show Material materials with Conductividad térmica of 209.0 - 222.0 W/(m·K) | Typical for Cast 1xx.x Series Aluminium |
Temperatura de fusión | 643.0 - 657.0 °C Show Material materials with Temperatura de fusión of 643.0 - 657.0 °C | Typical for Cast 1xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Circonio | 0.15 - 0.25 % Show Material materials with Circonio of 0.15 - 0.25 % | T5 | GB 1173 |
Hierro | 0.60 % Show Material materials with Hierro of 0.60 % | T5 | GB 1173 |
Magnesio | 0.15 - 0.25 % Show Material materials with Magnesio of 0.15 - 0.25 % | T5 | GB 1173 |
Manganeso | 0.9 - 1.2 % Show Material materials with Manganeso of 0.9 - 1.2 % | T5 | GB 1173 |
Níquel | 0.2 - 0.3 % Show Material materials with Níquel of 0.2 - 0.3 % | T5 | GB 1173 |
Silicona | 1.6 - 2.0 % Show Material materials with Silicona of 1.6 - 2.0 % | T5 | GB 1173 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | T5 | GB 1173 |